Defect-mediated magnetic performance in cold-compacted and post-annealed MnAl alloys
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T45 · pp.86 · 2026
- 피인용
- Web of Science 0Scopus 0
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2024 6.6
- ISSN
- 2238-7854
저자
- 장보초제1저자Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Song, YoungwoonKorea Inst Mat Sci, Nano Mat Res Div, Chang Won 51508, South Korea
- 정성Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- 주천홍Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Choi, Chul-JinKorea Inst Mat Sci, Nano Mat Res Div, Chang Won 51508, South Korea
- 리오이룬교신저자Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Si, PingzhanKorea Inst Mat Sci, Nano Mat Res Div, Chang Won 51508, South Korea
- Park, Jihoon교신저자Korea Inst Mat Sci, Nano Mat Res Div, Chang Won 51508, South Korea
초록
Rare-earth-free L10 tau-MnAl is attractive for functional magnetic applications, but its magnetic response is strongly coupled to phase constitution, deformation defects and texture developed during processing. Here, undoped Mn54Al46 powders and bulk compacts were prepared by melt spinning, jet milling, powder annealing, 4 GPa cold compaction and post-annealing. Jet milling produced fine epsilon-MnAl precursor powders with a defect-rich internal structure. Among all samples, powder annealing at 460 degrees C gave the highest tau-phase fraction of approximately 88% and the largest high-field magnetization measured at 2.5 T (M2.5T). High-pressure cold compaction increased the coercivity (mu 0Hc) to 0.49-0.51 T, but reduced the remanent magnetization (Mr) and M2.5T, consistent with severe lattice distortion, disrupted magnetic continuity between particles and possible local tau-phase destabilization. Post-annealing at 460 degrees C for 30 min partially relaxed the deformation structure, reducing the average KAM value and the estimated geometrically necessary dislocation density while strengthening the (001)-related preferred orientation from 5.32 to 9.59 multiples of a random distribution (M.R. D.). Consequently, M2.5T recovered to 65-66 Am2 & sdot;kg-1 and Mr increased to 36-38 Am2 & sdot;kg-1, while mu 0Hc remained 0.39-0.43 T. These results illustrate that the magnetic response of cold-compacted tau-MnAl is governed by a tradeoff between deformation-assisted pinning and annealing-induced structural recovery.
키워드
tau-MnAlCold compactionPost-annealingCoercivityDefect recoveryPHASE-TRANSFORMATIONREVERSAL PROCESSESTAU-PHASECOERCIVITYMICROSTRUCTUREPOWDERTWIN