Raman-calibrated image-based screening of ambient aging in CVD-grown HfS2 thin films
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널
- MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING217 · #111122 · 2027
- 피인용
- Web of Science 0Scopus 0
- FWCI (Scopus)
- 0
- ISSN
- 1369-8001
저자
- 전용철제1저자Pusan Natl Univ, Coll Engn, Major Intellectual Property Convergence, Busan 46241, South Korea
- Hwang, JuchanJeonbuk Natl Univ, Div Adv Mat Engn, Jeonju 54896, South Korea
- Tan, Chee LeongPortland State Univ, Dept Elect & Comp Engn, Portland, OR 97201 USA
- Park, Kwangwook교신저자Jeonbuk Natl Univ, Div Adv Mat Engn, Jeonju 54896, South Korea
초록
HfS2 is a layered semiconductor for electronic and optoelectronic applications, but humidity-assisted native oxidation limits its ambient stability. Raman spectroscopy probes HfS2 degradation but is time-consuming and condition-sensitive. Here, we revisit a previously reported HfS2 aging dataset to develop a Raman-calibrated image-based framework for rapid, non-destructive screening of CVD-grown HfS2 films on c-plane sapphire. Photographs collected under a documented configuration yielded predefined color, histogram, texture, and spatial descriptors. A simple, interpretable regression using only CIE Lab b* with physical-range clipping achieved a within-library, query-excluded leave-one-day-out RMSE of 6.78 days for 21 queries from three optically evolving conditions: native HfS2 at 35% and 70% RH and PMMA-capped HfS2 at 70% RH. The b*-based model performed comparably to kNN (7.70 days) and significantly better than a no-information pool-mean baseline (9.84 days, p = 0.0030), indicating that more complex estimators provided no clear benefit in the present dataset. Under leave-one-pair-out evaluation of 20 image-Raman pairs, the combined image-derived estimate showed a trend-level relationship with measured normalized A1g intensity (R2 = 0.600), while Delta E gave the best individual result (R2 = 0.701). The framework identified its limits: severe degradation of native HfS2 at 70% RH was underestimated, whereas Al2O3-encapsulated HfS2 showed insufficient optical evolution for reliable chronological estimation. Accordingly, this material-and configuration-specific method is a proof-of-concept screening framework, not a universal dating model or a substitute for Raman spectroscopy. Within this scope, controlled photography provides interpretable pre-screening of broad aging states and prioritizes samples for Raman or chemical analysis.
키워드
HfS2Native oxidationRaman-calibrated imagingThin-film agingImage-based screeningSCATTERINGMONOLAYERZRS2