Substrate effects in VMoCe/TiO2 monolithic NH3-SCR catalysts under high-NOx model conditions relevant to ammonia co-firing power exhaust
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING14(5) · 2026
- 피인용
- Web of Science 0Scopus 0
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2024 7.2
- ISSN
- 2213-2929
저자
- Lee, Jong-Hoon제1저자Korea Inst Ind Technol, Low Carbon Energy Grp, Ulsan, 44413, South Korea
- Lee, Min EuiKorea Elect Power Corp Res Inst, Energy & Environm Lab, Daejeon 34056, South Korea
- Kim, HyejinKorea Inst Ind Technol, Low Carbon Energy Grp, Ulsan, 44413, South Korea
- Kim, Hee SooKorea Inst Ind Technol, Low Carbon Energy Grp, Ulsan, 44413, South Korea
- 임동하교신저자Pusan Natl Univ, Grad Sch Hydrogen & Next Energy Convergence, Busan 46241, South Korea
초록
High-NOx ammonia co-firing exhaust requires compact selective catalytic reduction systems that retain activity under sulfur- and water-containing conditions. This study compared SUS304 stainless-steel and cordierite ceramic monolith configurations coated with VMoCe/TiO2 at closely matched washcoat loadings under literature-informed synthetic-gas conditions. The feed contained 1000 ppm NO, 1000 ppm NH3, 8 vol% O2, and 10 vol% H2O at a nominal gas hourly space velocity of 20,000 h−1; 100 ppm SO2 was introduced during the poisoning and time-on-stream tests. After coating, the metallic configuration retained a larger open frontal area and smaller total coated-wall thickness, and the metallic holder–monolith assembly showed a 14–35% lower pressure drop than the ceramic configuration. At 350 °C, NO conversion reached 99.2% and 94.5% for the metallic and ceramic configurations, respectively. The apparent activation energies were 26.01 ± 1.25 and 27.35 ± 1.36 kJ mol−1, respectively, with substantially overlapping 95% confidence intervals, indicating comparable reactor-scale apparent kinetic behavior within the regression uncertainty. After sequential SO2/H2O exposure, activity recovery at 350 °C reached 97.7% and 95.0%, while post-reaction X-ray photoelectron spectroscopy showed residual surface sulfur concentrations of 1.1 and 1.8 at%, respectively. During 250 h of continuous SO2/H2O-containing operation at 300 °C, NO conversion remained above 92.4% for the metallic configuration and approximately 87.8% for the ceramic configuration. These results show distinct configuration-level hydraulic, catalytic, surface-sulfur, and time-on-stream responses under the tested conditions; validation using actual exhaust, bare-substrate controls, and broader application-specific operating conditions remains necessary.
키워드
Ammonia co-firingCordierite monolithMetallic monolithNH3-SCRSurface-sulfur responseTime-on-stream stability