Microstructure and mechanical properties of tungsten carbide-reinforced commercially pure Ti matrix composite coatings deposited by laser cladding

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q1Scopus Q1
피인용
Web of Science 0Scopus 0
FWCI (Scopus)
0
JCR IF
JCR 2024 6.6
ISSN
2238-7854

저자

  1. 이승민제1저자Pusan Natl Univ, Sch Mech Engn, Busan 46241, South Korea
  2. Kim, Chung-SooEloi Mat, Suwon 16229, South Korea
  3. Kim, JungsubKorea Inst Ind Technol, 3D Printing Mfg Proc Ctr, Ulsan 44776, South Korea
  4. 박석희교신저자Pusan Natl Univ, Sch Mech Engn, Busan 46241, South Korea
  5. Ha, Jeonghong교신저자Korea Inst Ind Technol, 3D Printing Mfg Proc Ctr, Ulsan 44776, South Korea

초록

Commercially pure titanium (CP Ti) exhibits excellent corrosion resistance and formability. However, its relatively low hardness limits its use in applications requiring wear resistance. In this study, tungsten carbide (WC)-reinforced CP Ti composite coatings were deposited on CP Ti (Grade 2) substrates via laser cladding using a laser-directed energy deposition system without preheating. A representative process condition of 2300 W and 500 mm/min was selected based on the dilution ratio to avoid excessive dilution while ensuring metallurgical bonding, and no visible cracks were observed after penetrant testing and polished surface examination. Microstructural and phase analyses showed that WC addition increased the retained β-Ti fraction through W dissolution and β stabilization, while promoting the in situ formation of TiC carbide phases around partially unmelted WC particles. Consequently, the microhardness increased from 242 HV at 0 wt% WC to 511 HV at 30 wt% WC. Ball-on-disk tests revealed that increasing the WC content significantly reduced the wear depth and improved wear resistance, although the coefficient of friction exhibited greater fluctuations. Additional SEM/EDS analysis of the worn WC counterface balls showed that W-rich debris could originate from the coating, the counterface ball, or both, indicating debris-assisted three-body abrasion at higher WC contents. Potentiodynamic polarization tests in 3.5 wt% NaCl solution further showed improved corrosion resistance for the WC-containing coatings. These results demonstrate that WC addition effectively controls β-Ti stabilization, carbide formation, hardness, wear behavior, and corrosion resistance in laser-cladded CP Ti-WC composite coatings.

키워드

Commercially pure titaniumLaser claddingMechanical propertiesMetal matrix compositesMicrostructureTungsten carbide