Positive Aging-Free Quantum Dot Light-Emitting Diodes Enabled by Single-Source Chloride-Doped ZnMgO Electron Transport Layers
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- SMALL22(37) · 2026
- 피인용
- Web of Science 2Scopus 2
- FWCI (Scopus)
- 0.88
- JCR IF
- JCR 2024 12.1
- ISSN
- 1613-6810
저자
- 이재엽제1저자Pusan Natl Univ, Dept Elect Engn, Pusan, South Korea
- 배예윤Pusan Natl Univ, Dept Elect Engn, Pusan, South Korea
- 이경은Pusan Natl Univ, Dept Elect Engn, Pusan, South Korea
- Jung, Woon HoSungkyunkwan Univ SKKU, Ctr Artificial Atoms, Dept Energy Sci, Suwon, Gyeonggi Do, South Korea
- Lee, HyeonjunSungkyunkwan Univ SKKU, Ctr Artificial Atoms, Dept Energy Sci, Suwon, Gyeonggi Do, South Korea
- Kim, Byong JaeSungkyunkwan Univ SKKU, Ctr Artificial Atoms, Dept Energy Sci, Suwon, Gyeonggi Do, South Korea
- Kim, HyoungjunSungkyunkwan Univ SKKU, Ctr Artificial Atoms, Dept Energy Sci, Suwon, Gyeonggi Do, South Korea
- 김건우Pusan Natl Univ, Inst Environm & Energy, Sch Chem Engn, Busan, South Korea
- 정병국Pusan Natl Univ, Inst Environm & Energy, Sch Chem Engn, Busan, South Korea
- Lim, JaehoonSungkyunkwan Univ SKKU, Ctr Artificial Atoms, Dept Energy Sci, Suwon, Gyeonggi Do, South Korea
- 노정균교신저자Pusan Natl Univ, Dept Elect Engn, Pusan, South Korea
초록
Colloidal quantum dot light-emitting diodes (QD-LEDs) offer narrowband, color-pure emission, solution processability, and wavelength tunability for next-generation displays. However, commercialization is hindered by positive aging-a storage-driven drift in which device external quantum efficiency (EQE) increases for several days before peaking, reflecting slow interfacial trap passivation in oxide electron-transport layers (ETLs). This drift delays qualification, complicates calibration, and degrades device-to-device uniformity because the as-fabricated performance does not represent the final state. Here, we suppress positive aging by pre-stabilizing ZnMgO ETLs via single-source chloride doping (MgCl2), which mitigates oxygen vacancy (OV)-related defect signatures. Time-dependent X-ray photoelectron spectroscopy, single-carrier device measurements, and steady-state/time-resolved QD photoluminescence show that undoped ZnMgO undergoes gradual defect passivation during storage, whereas Cl-doped ZnMgO remains nearly time-invariant. As a result, devices with Cl-doped ZnMgO reach peak EQE at day 0 and maintain it during storage, while devices with undoped ZnMgO require several days to reach peak efficiency. In addition, as-fabricated QD-LEDs employing Cl-doped ZnMgO exhibit approximate to 1.8 & times; higher peak EQE and approximate to 1.3 & times; longer operational lifetime than undoped controls, with negligible positive aging signatures. This intrinsic ETL stabilization enables day-0 calibration, improves uniformity and yield, and removes the need for storage-driven conditioning-identifying single-source chloride doping as a practical route to robust ZnMgO ETLs for display applications.
키워드
electron transport layerpositive agingquantum dot light emitting diodesquantum dotZnMgO nanoparticlesPERFORMANCE