Selective separation and recovery of strontium from seawater reverse osmosis brine using sequential oxalate precipitation and ion exchange
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q4Scopus Q3
- 저널
- DESALINATION AND WATER TREATMENT326 · 2026
- 피인용
- Web of Science 3Scopus 3
- FWCI (Scopus)
- 2.59
- JCR IF
- JCR 2024 1
- ISSN
- 1944-3994
저자
- Moon, Jeong-ki제1저자Res Inst Ind Sci & Technol RIST, Environm & Energy Res Lab, Pohang 37673, Gyeongsangbug, South Korea
- Choi, SangkiRes Inst Ind Sci & Technol RIST, Environm & Energy Res Lab, Pohang 37673, Gyeongsangbug, South Korea
- Ahn, TaebumKorea Zinc Co, Res & Dev Team 2, Ulsan 44997, South Korea
- Kwon, Hyuk-JunGyeongbuk Dev Inst, Spatial &Environment Res Lab, Yecheon 36849, Gyeongsangbug, South Korea
- 이우림교신저자Pusan Natl Univ, Dept Bioenvironm Energy, Miryang 50463, Gyeongsangnam D, South Korea
초록
Seawater desalination effectively produces fresh water, yet brine byproducts raise significant environmental concerns. Strontium, a valuable resource in brine, is increasingly sought after due to diminishing terrestrial mineral sources. However, its recovery is challenging because strontium ion (Sr2+) and calcium ion (Ca2+) exhibit similar physicochemical behaviors in the aqueous phase, necessitating advanced recovery technologies. This study proposes an integrated recovery process for seawater reverse osmosis (SWRO) brine combining oxalate-based precipitation and ion exchange. In the pretreatment stage, NaOH and oxalate were employed to sequentially remove magnesium and calcium interferences. Specifically, oxalate addition at a 1.6 molar ratio relative to Ca2+ preferentially precipitated calcium, drastically increasing the [Sr2+]/[Ca2+] ratio from 0.016 to 2.5, indicating a notable enhancement in Sr2+ relative to Ca2+. For the enrichment of Sr2+ from the pretreated solution, an ion-exchange column was employed. Two consecutive concentration cycles yielded a Sr-enriched solution exceeding 4 g/L. A post-IEX Ca2+ removal step further reduced residual calcium, achieving a maximum [Sr2+]/[Ca2+] ratio of 28.6, with a Sr2+ concentration of approximately 2 g/L. These results demonstrate that an integrated process using sequential oxalate-based precipitation and ion exchange achieves high efficiency in Ca2+ removal, enhancing the overall feasibility of the Sr2+ recovery process.
키워드
Ion exchangeOxalate precipitationResource recoverySeawater reverse osmosis (SWRO) brineSelective separationStrontium recovery