Recent advances in medium-manganese steel: a review of key findings, challenges, and future perspectives

문서 유형
연구출판물 · 리뷰논문
등재
SCIEScopus
저널 순위
JCR Q2Scopus Q1
저널
JOURNAL OF MATERIALS SCIENCE60(23) · pp.9447 · 2025
피인용
Web of Science 25Scopus 25
FWCI (Scopus)
1.32
JCR IF
JCR 2024 3.9
ISSN
0022-2461

저자

  1. Mohapatra, Sudipta제1저자Jeonbuk Natl Univ, Convers Engn Grad Sch, Dept Energy Storage, Div Adv Mat Engn, Jeonju 54896, South Korea
  2. Satpathy, BangmayaIndian Inst Technol, Dept Met Engn & Mat Sci, Bombay 400076, Mumbai, India
  3. Sarkar, ArnabNatl Inst Technol Rourkela, Dept Met & Mat Engn, Rourkela 769008, Odisha, India
  4. Kumar, SumanIndian Inst Technol Kharagpur, Dept Met & Mat Engn, Kharagpur 721302, West Bengal, India
  5. 아이치 샤티야브러타Pusan Natl Univ, Sch Comp Sci & Engn, Busan 46241, South Korea
  6. Oh, Min-Suk교신저자Jeonbuk Natl Univ, Convers Engn Grad Sch, Dept Energy Storage, Div Adv Mat Engn, Jeonju 54896, South Korea

초록

This review paper aims to provide an overview of the advancements achieved with medium-manganese steel (MMnS) for its application in the automobile industry. The review work will cover various aspects, including chemical composition design, the correlation between structure and properties, deformation mechanism, effect of strain rate, electrochemical behavior, wear, and weldability response. We classify MMnS as third-generation advanced high-strength steels. The automotive industry widely utilizes these steels due to their superior properties and performance. Various factors, including the phase composition and distribution within the microstructure, the volume fraction, size, and morphology of phase constituents, and the stability of metastable constituents, influence the tensile properties of MMnS. High transformation-induced plasticity effect and dislocation density increase strength and ductility at low strain rates. Dynamic impact properties of MMnS depend on ductile-to-brittle transition temperature, chemical composition, and austenite mechanical stability. Due to low current density, charge transfer resistance, corrosion rate, and austenite manganese concentration, higher-temperature annealing resists corrosion better. MMnS can be welded using friction stir welding to retain their mechanical properties and prevent martensitic transformation. The present article provides an insight into the recent works, new sector applications, industrial-scale feasibility, long-term phase stability, future scope, and challenges of MMnS.

키워드

MEDIUM-MN STEELSTRESS-CORROSION CRACKINGWORK-HARDENING BEHAVIORSTACKING-FAULT ENERGYINTERCRITICAL ANNEALING TEMPERATUREINDUCED MARTENSITIC-TRANSFORMATIONRETAINED AUSTENITE CHARACTERISTICSMECHANICAL PROPERTY RELATIONSHIPHIGH DUCTILITY COMBINATIONHYDROGEN-INDUCED CRACKING