High-Temperature Properties of LP-DED Additive Manufactured Ferritic STS 430 Deposits on Martensitic STS 410 Base Metal
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q1
- 저널
- MICROMACHINES16(5) · #494 · 2025
- 피인용
- Web of Science 3Scopus 3
- FWCI (Scopus)
- 0.4
- JCR IF
- JCR 2024 3
- ISSN
- 2072-666X
저자
- 변삼섭제1저자Pusan Natl Univ, Dept Mat Sci & Engn, Busandaehak Ro 63beon Gil, Busan 46241, South Korea
- Kang, Hyun-Ki교신저자R&D Ctr, Turbo Power Tech, 107 Dasan Ro, Busan 49488, South Korea
- 강남현Pusan Natl Univ, Dept Mat Sci & Engn, Busandaehak Ro 63beon Gil, Busan 46241, South Korea
- Lee, SeunghunTESONE Co Ltd, Welding & Joining Dev Team, 37 Nakdong Daero 550beon Gil, Busan 49315, South Korea
초록
The aim of this work is to study the phase transformations, microstructures, and mechanical properties of ferritic stainless steel (FSS) 430 deposits on martensitic stainless steel (MSS) 410 base metal (BM) using laser powder-directed energy deposition (LP-DED) additive manufacturing. The LP-DED additive manufactured FSS 430 deposits on MSS 410 BM underwent post-heat treatment at 815 degrees C and 980 degrees C for 1 h, respectively. The analyses of phase transformations and microstructural evolutions of LP-DED FSS 430 on MSS 410 BM were carried out using X-ray diffraction, SEM, and EBSD. The highest strain was observed at the coarsened chromium carbide (Cr23C6) in the joint interface between AM FSS 430 and MSS 410 MB. This contributed to localized lattice distortion and mismatch in crystal structure between chromium carbide and the surrounding ferrite. Tensile strength properties at elevated temperatures were discussed to investigate the effects of the different post-heat treatments. The tensile properties of the as-built samples including tensile strength of about 550 MPa and elongation of about 20%, were the same as those of the commercial FSS 430 material. Tensile properties at 500 degrees C indicated a modest increase in tensile strength to 540-550 MPa. The specimens heat treated at 980 degrees C retained higher tensile strength than those heat treated at 815 degrees C. This would be attributed to the grain refinement from prior LP-DED microstructure and chromium carbide coarsening at higher heat treatment, which can increase dislocation density and yield harder mechanical behavior.
키워드
additive manufacturingdirected energy depositionferritic stainless steel 430martensitic stainless steel 410chrome carbide precipitationSTAINLESS-STEELRESISTANCE