- Jin Hyok Lee제1저자한국소재융합연구원
- Myung Chan Choi한국소재융합연구원
- 윤유미한국소재융합연구원
- Yongsu Jo한국소재융합연구원
- Yongwon Cho한국소재융합연구원
- Sung Han ParkAgency for Defense Development
- 김원호Pusan National University
- 배종우교신저자한국소재융합연구원
초록
In this study, we observed the effect of thermal degradation on the low-temperature sealing capability. A large- sized CR O-ring of 90.0 mm inner diameter and 7.0 mm cross-sectional diameter was used. In FT-IR spectroscopy, the aged CR O-ring, CR-10, showed a carboxyl group upon oxidation. Through oxidation, the sealing force of the aged CR O-rings decreased with an increase in the degree of degradation. As the degree of degradation increased, the 10% compressive modulus had higher values at each relative position. Oxidation was caused by oxygen diffusion to the CR interface. As the degree of degradation increased, glass transition temperature (Tg) was increased, and tan δ was decreased. CR-10 showed -44.0℃ of Tg and 0.89 of tan δ. With an increase in the degree of degradation, the mobility of the CR decreased and showed a slow recovery rate at low temperatures. All specimens showed lower temperature retraction 10 (TR10) than Tg with 2.0-2.5℃ difference. The gas leakage temperature increased with the degree of degradation. This coincided with Tg and TR10 tendency. Under Tg and TR10, CR could still exhibit viscoelastic properties and could be used as a seal. At the gas leakage temperature, the CR changed to a glassy state, and leakage occurred.
키워드
CR O-ringLow temperature sealing capabilityTemperature retraction (TR)Glass transition temperature (Tg)Modulus profiles