LNG 화물창 하부 플라이우드 구조건전성에 미치는 함수율의 영향
Effect of Moisture Content on the Structural Integrity of the Bottom Plywood in the LNG Cargo Containment System
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCI
- 저널 순위
- KCI Q1
- 저널
- 대한조선학회 논문집62(1) · pp.1 · 2025
- 피인용
- KCI 0
- ISSN
- 1225-1143
저자
초록
Plywood is an orthotropic material made from wood. Due to its high strength and durability, it is used in the insulation systems of LNG cargo containment system, both at the top and bottom. In the actual operational environment of LNG cargo containment system, dry nitrogen with a dew point below –45 ℃ is purged at atmospheric pressure to inert the insulation system and remove moisture. During this process, the moisture content of plywood continually decreases. Wood materials, such as plywood, exhibit varying mechanical properties depending on moisture content, with reduced elongation and bending strength at lower moisture levels. In particular, the bottom plywood for insulation panel is vulnerable to shear failure due to sloshing impact loads at the mastic bonding area; thus, sufficient structural strength must be ensured. Therefore, evaluating mechanical performance and failure behavior at low moisture content levels is essential. This study proposed a panel testing method for evaluating the deformation and failure behavior of bottom plywood. Based on experimental results considering actual operational environments, it was observed that dried plywood exhibits increased susceptibility to failure. In particular, plywood placed parallel to the mastic bonding direction presents a significantly higher risk of structural failure.
키워드
Liquefied natural gas(액화천연가스)Plywood(플라이우드)Mechanical properties(기계적 물성)Moisture content(함수율)
식별자
- KCI
- ART003173760



로그인
연구물 목록으로