Effect of δ-ferrite and strain-induced on hydrogen embrittlement of STS 308 L and STS 316 L all-weld metals

Effect of δ–ferrite and strain-induced martensite on hydrogen embrittlement of STS 308 L and STS 316 L all-weld metals

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q1Scopus Q1
저널
CORROSION SCIENCE231 · 2024
피인용
Web of Science 20Scopus 21
FWCI (Scopus)
1.61
JCR IF
JCR 2023 7.4
ISSN
0010-938X

저자

  1. 최동현제1저자Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
  2. 남지민Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
  3. 문병록Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
  4. 수라브 쿠마 사하Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
  5. 유재석Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
  6. Park, Jong MinWelding Engn R&D Team, Hanwha Ocean, Geoje Si, South Korea
  7. Yun, Kwang HeeWelding Engn R&D Team, Hanwha Ocean, Geoje Si, South Korea
  8. 강남현교신저자Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea

초록

The susceptibility of multipass flux-cored arc welds of STSs 308 L and 316 L to hydrogen embrittlement (HE) was investigated at various temperatures. Cracks predominantly initiated and propagated along the δ-ferrite in the interdendritic region at 25 °C. δ-ferrite served as preferred hydrogen trap sites, and the δ/γ boundary became the stress concentration site. At −100 °C, STSs 308 L and 316 L exhibited high susceptibility to HE owing to strain-induced martensite formation, providing additional hydrogen trap sites and dislocation accumulation. Despite strain-induced martensite actively transformed at −196 °C, the HE disappeared owing to the sluggish diffusion of hydrogen to stress-concentrated areas.