본문 바로가기

Formation behavior of anodizing films on various aluminum alloys in oxalic acid solution

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q2Scopus Q1
피인용
Web of Science 12Scopus 13
FWCI (Scopus)
1.12
JCR IF
JCR 2023 4.3
ISSN
0254-0584

저자

  1. Pham, Hien Van제1저자Korea Inst Mat Sci, Surface & Nano Mat Div, 797 Changwon Daero, Chang Won 51508, Gyeongnam, South Korea
  2. 권두영Pusan Natl Univ, Dept Mat Sci & Engn, 2 Busandaehak Ro,63beon Gil, Busan 46241, South Korea
  3. 김주석Pusan Natl Univ, Dept Mat Sci & Engn, 2 Busandaehak Ro,63beon Gil, Busan 46241, South Korea
  4. 김리경Pusan Natl Univ, Dept Mat Sci & Engn, 2 Busandaehak Ro,63beon Gil, Busan 46241, South Korea
  5. Moon, Sungmo교신저자Korea Inst Mat Sci, Surface & Nano Mat Div, 797 Changwon Daero, Chang Won 51508, Gyeongnam, South Korea

초록

The formation behavior of anodic aluminum oxide (AAO) films on various aluminum alloys, was studied in 6 wt% oxalic acid solution. There were observed two different voltage-time behaviors with a sharp peak in the initial stage of galvanostatic anodizing for pure Al, AA1050 and AA5052 (group 1), and with voltage plateaus instead of a peak for AA7075, AA6061 and AA2024 (group 2). AAO film growth rate was found to be higher for the group 1 specimens than the group 2 alloys. Two different anodizing films appeared, with regularly ordered cylindrical nano-pores for the group 1 specimens and irregularly distorted nano-pores along with numerous nano-cavities for the group 2 alloys. As the anodizing time increased, the AAO films on the group 1 specimens became darkened, while those on the group 2 alloys were not darkened but only changed in color. In addition, the surface hardness of the AAO films was much higher on the group 1 specimens than the group 2 alloys.

키워드

Aluminum alloyAnodic oxide filmAnodizingHardnessOxalic acid anodizingCORROSION-RESISTANCESULFURIC-ACIDOXIDE LAYERSMECHANISMANODIZATIONGENERATIONDEPOSITIONPARTICLESOXIDATIONGROWTH

식별자

Scopus EID
2-s2.0-85183140578
WoS UID
001172575900001