Robust Pr6O11 infiltration for La0.6Sr0.4Co0.2Fe0.8O3-δ cathode performance enhancement on electrolyte supported solid oxide fuel cells
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q3Scopus Q2KCI Q4
- 저널
- CURRENT APPLIED PHYSICS59 · pp.39 · 2024
- 피인용
- Web of Science 9Scopus 10KCI 0
- FWCI (Scopus)
- 0.79
- JCR IF
- JCR 2023 2.4
- ISSN
- 1567-1739
저자
- 김용재제1저자Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
- 뤄 준메이Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
- 박서현Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
- 안세현Pusan Natl Univ, Dept Mech Engn, Busan 46241, South Korea
- 염은섭Pusan Natl Univ, Dept Mech Engn, Busan 46241, South Korea
- 리오이룬교신저자Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
초록
In this study, the infiltration of a novel electrocatalyst, Praseodymium oxide (Pr6O11), has successfully enhanced solid oxide fuel cell (SOFC) performance via simple infiltration method. Pristine Lanthanum strontium cobalt ferrite (LSCF) screen printed on a electrolyte supported SOFC button cell showed peak power density of 0.086 W/cm2 at 800 °C, infiltrating 0.1 mol/L of Pr6O11 precursor into the LSCF cathode increased performance by 16.3 % by recording a 0.100 W/cm2 peak power density and infiltrating higher concentration of 1 mol/L Pr6O11 precursor further increased power density to 0.118 W/cm2, a 37.2 % improvement. Although increasing temperature lowered the effectiveness of the electrocatalyst, 1 mol/L Pr6O11 precursor infiltrated LSCF still showed the highest peak power density overall with 0.237 W/cm2 at 900 °C, a 13.9 % increase from pristine LSCF's 0.208 W/cm2 at the same temperature. The results confirm that increasing Pr6O11 precursor concentration in infiltration solution is an effective way for improving SOFC performance.
키워드
Cathode performanceElectrocatalyst infiltrationElectrolyte supported solid oxide fuel cellLSCFPraseodymium oxidePOWER-GENERATIONSURFACE EXCHANGEDIFFUSION
식별자
- Scopus EID
- 2-s2.0-85181718133
- WoS UID
- 001165025700001
- KCI
- ART003063681



로그인
연구물 목록으로