본문 바로가기

Phase Formation, Residual Stress, and Surface Energy of Carbon-Doped TiZrN Coatings

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q3Scopus Q2
저널
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE33(24) · pp.13993 · 2024
피인용
Web of Science 1Scopus 2
FWCI (Scopus)
0.18
JCR IF
JCR 2023 2.2
ISSN
1059-9495

저자

  1. 이승재제1저자Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
  2. 김성훈Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
  3. 홍은표Korea Testing Lab, Mech & Mat Technol Ctr, Jinju 52852, South Korea
  4. Choi, YoungkueKorea Testing Lab, Mech & Mat Technol Ctr, Jinju 52852, South Korea
  5. 조현Pusan Natl Univ, Dept Nanomechatron Engn, Busan 46241, South Korea
  6. Jo, IlgukDong Eui Univ, Dept Adv Mat Engn, Busan 47340, South Korea
  7. 이희수교신저자Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea

초록

We investigated the relationship between the surface energy, phase formation, residual stress, and wettability of carbon-doped TiZrN coatings. Carbon-doped TiZrN coatings were prepared via laser ablation by controlling the thickness of the carbon paste. The crystal structure analysis revealed that the (111) plane peak shifted to a lower angle as the paste thickness increased. Lattice expansion was confirmed through Rietveld refinement, and the lattice constant of the coating increased from 4.17 to 4.41 Å. Based on X-ray photoelectron spectroscopy, it was confirmed that the formation of carbide (TiC, ZrC) phase was 4.85% for a paste thickness of 100 μm, and 12.10% for a paste thickness of 180 μm. The TiC/ZrC ratio also increased with paste thickness. The increase in carbide formation was attributed to the initial carbon concentration, whereas the increase in the TiC/ZrC ratio was ascribed to the reduction of high-energy carbon, which was sufficient to form ZrC bonds by plasma shielding. The residual stress was calculated to increase from 4439 to 5861 MPa using the sin2 ψ method. The contact angle of water decreased from 95.9° to 74.75° and that of diiodomethane decreased from 46.75° to 36.65° after carburization. With carburization, an improvement in wettability was observed for both polar and dispersive liquids, with the surface energy increasing from 36.42 to 46.24 mN/m.

키워드

carbides formationcarbon-doped TiZrN coatingscarburization behaviorpolar and nonpolar surface energiesresidual stressWEARTIN

식별자

Scopus EID
2-s2.0-85179677778
WoS UID
001124699800003