Microstructure and mechanical properties of adjustable-ring-mode laser welded and hot-stamped Al–Si coated boron steel joints
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T28 · pp.844 · 2024
- 피인용
- Web of Science 21Scopus 22
- FWCI (Scopus)
- 2
- JCR IF
- JCR 2023 6.2
- ISSN
- 2238-7854
저자
- 전현욱제1저자Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
- 김재득Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
- Cheon, JooyongKorea Inst Ind Technol, Adv Forming Proc R&D Grp, Ulsan 44413, South Korea
- Kim, JaehunKorea Inst Ind Technol, Adv Forming Proc R&D Grp, Ulsan 44413, South Korea
- Park, Yeong-DoDong Eui Univ, Dept Adv Mat Engn, Busan 47227, South Korea
- 김양도교신저자Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
- Ji, Changwook교신저자Korea Inst Ind Technol, Adv Forming Proc R&D Grp, Ulsan 44413, South Korea
초록
The microstructure and mechanical properties of adjustable-ring-mode (ARM) laser-welded, hot-stamped 22MnB5 steel joints were analyzed and compared with those of Al–Si coated 22MnB5. Al segregation into the fusion zone (FZ) was suppressed by a ring beam introduced via ring-beam-mode (RBM) and dual-beam-mode (DBM) laser welding. Dilution of the Al–Si coating in the FZ induced α-ferrite formation during hot stamping. After hot stamping, the α-ferrite fraction in the FZ decreased (from 23 vol% to 4.27 vol%) more than that in the center-beam-mode (CBM) welded joints owing to the ring beam. Electron backscattered diffraction analysis indicated the distribution of high-density and uniform geometrically necessary dislocations, which caused coordinated deformation in the martensite grains, in the RBM and DBM FZs. The average microhardness in the FZ in the tailor-welded blank (TWB) joints was ∼30–40 HV lower than that in the RBM and DBM welded base metal (480 HV) and that in the FZ of the CBM reduced to 295 HV because of the formation of a large amount of ductile α-ferrite. The tensile strength and elongation of the TWB joint in the CBM were ∼989 MPa and 1.1 %, respectively, which were significantly lower than those of the RBM (1245 MPa and 1.96 %, respectively) and DBM (1321 MPa and 2.12 %, respectively). Finally, the 22MnB5 steel sheets were subjected to ARM laser welding without removing the coating layer to evaluate the effect of the ring beam on Al segregation suppression in the FZ and mechanical properties of the TWB joints.
키워드
Al–Si coatedARM laserHot-stampedMechanical propertiesMicrostructureRing beamPRESS-HARDENED STEELTAILORED BLANKSDELTA-FERRITEEVOLUTIONRECRYSTALLIZATION
식별자
- Scopus EID
- 2-s2.0-85179587205
- WoS UID
- 001139872600001



로그인
연구물 목록으로