본문 바로가기

Materialization of the Heat-Affected Zone with Laser Tailor-Welded HPF 22MnB5 Steel Using FLD and the Fracture Displacement Method in FE Simulation

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q2Scopus Q1
저널
METALS13(10) · 2023
피인용
Web of Science 3Scopus 3
FWCI (Scopus)
0.21
JCR IF
JCR 2022 2.9
ISSN
2075-4701

저자

  1. 전현종제1저자Pusan Natl Univ, Sch Mech Engn, 30 Jangjeon Dong, Busan 46241, South Korea
  2. Jin, Chul KyuKyungnam Univ, Sch Mech Engn, 7 Kyungnamdaehak Ro, Changwon Si 51767, South Korea
  3. 이민식교신저자Pusan Natl Univ, Sch Mech Engn, 30 Jangjeon Dong, Busan 46241, South Korea
  4. Lim, Ok DongAutogen Co Ltd, 2611-1 Jeongwang Dong, Siheung Si 15089, South Korea
  5. Kang, Nam SuAutogen Co Ltd, 2611-1 Jeongwang Dong, Siheung Si 15089, South Korea

초록

Using a tailor-welded blank (TWB) and hot-press forming (HPF), a 22MnB5 blank was surface-treated under four conditions. The penetration rates of the FexAly compounds under the four surface-treatment conditions were investigated, and the hardness values were measured. A finite element (FE) simulation was performed for the characteristics of the heat-affected zone (HAZ), using the hardness value and results of previous researchers. In particular, the mechanical property settings of the mesh were designed to realize the conditions for the FexAly compounds in the HAZ. Fine meshing was performed by partitioning the HAZ sections. For the mechanical properties of the HAZ with the FexAly compounds, the strength was predicted from the hardness value, and the elongation values investigated by other researchers were used. The forming limit diagram, which was proportional to the elongation, was predicted. Specific elements were defined as the areas with FexAly compounds, which played the same role as impurities. Tensile TWB–HPF specimens with different HAZ characteristics under four surface-treatment conditions were fabricated. Experiments and FE simulations were performed and compared. Details are as follows: For loads, a minimum error rate of 3% and a maximum error rate of 6% were obtained. For displacement, a minimum error rate of 9% and a maximum error of 25% were obtained. The feasibility of the simulation was verified by comparing the simulation and experimental results. A match of more than 75% was obtained.

키워드

22MnB5Al–Si coating layerfinite element methodheat-affected zonehot-press formingtailor-welded blankAL-SIMECHANICAL-PROPERTIESMICROSTRUCTUREPLASTICITYCRACK