Green conversion of wood plastic composites: A study on gasification with an activated bio-char catalyst
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- INTERNATIONAL JOURNAL OF HYDROGEN ENERGY54 · pp.96 · 2024
- 피인용
- Web of Science 24Scopus 27
- FWCI (Scopus)
- 2.14
- JCR IF
- JCR 2023 8.1
- ISSN
- 0360-3199
저자
- Jeon, Sugyeong제1저자Univ Seoul, Sch Environm Engn, Seoul 02504, South Korea
- Farooq, AbidUniv Seoul, Sch Environm Engn, Seoul 02504, South Korea
- Lee, Im HackUniv Seoul, Sch Environm Engn, Seoul 02504, South Korea
- Lee, DoyeonHanbat Natl Univ, Dept Civil & Environm Engn, Daejeon 305719, South Korea
- Seo, Myung WonUniv Seoul, Sch Environm Engn, Seoul 02504, South Korea
- Jung, Sang-ChulSuncheon Natl Univ, Dept Environm Engn, Sunchun 57922, South Korea
- Hussain, MuridCOMSATS Univ Islamabad, Dept Chem Engn, Lahore Campus, Lahore, Pakistan
- Khan, Moonis AliKing Saud Univ, Coll Sci, Chem Dept, Riyadh 11451, Saudi Arabia
- Jeon, Byong-HunHanyang Univ, Dept Earth Resources & Environm Engn, Seoul, South Korea
- 장성호교신저자Pusan Natl Univ, Dept Bioenvironm Energy, Miryang 50463, South Korea
- Choi, Yong Jun교신저자Univ Seoul, Sch Environm Engn, Seoul 02504, South Korea
- Rhee, Gwang Hoon교신저자Univ Seoul, Dept Mech & Informat Engn, Seoul 02504, South Korea
- Park, Young-Kwon교신저자Univ Seoul, Sch Environm Engn, Seoul 02504, South Korea
초록
The excessive use of wood plastic composites (WPCs) at construction sites owing to their outstanding properties has caused serious disposal problems recently. Thermochemical conversions, such as pyrolysis and gasification, provide a solution for WPC disposal as a means of biofuel generation in an environmentally friendly manner. In this study, air gasification of WPCs was performed over activated bio-char-based catalysts for green valorization with the aim of achieving higher H2 generation. The KOH activation resulted in a significant increase in the Brunauer-Emmett-Teller surface area (14 times) and total pore volume (∼6.7 times), and KOH activated char was an excellent adsorbent for trapping tar, resulting in higher tar conversion into lighter hydrocarbons and H2. In addition, KOH-activated biochar showed the highest gas yield (69 wt%) and highest H2 selectivity (29.76 vol.%) compared to non-catalytic and non-activated bio-char catalysts. In contrast, an equivalence ratio of 0.20 was considered optimal over KOH-activated biochar for obtaining a higher H2 selectivity (29.76%) and minimum CO2 (17.08%). The increased catalyst/feedstock ratio from 0.1 to 0.2 also enhanced the conversion of WPC toward H2 generation (29.76%–35.93%). Finally, the Ni loading over KOH-activated biochar provided the highest H2 selectivity of 43% owing to the synergy of tar cracking, water gas shift reaction, and steam and dry reforming reactions. The increase in the H2 content of the product gas was significant because it increased the overall heating value and quality of the obtained gas. Largely, this study will be a stepping stone toward sustainable valorization of WPC over activated biochar-based catalysts for higher H2 generation.
키워드
Activated carbonBio-charGasificationWood plastic compositeBIOMASS GASIFICATIONBIOCHARKOHPERFORMANCEWASTECO2
식별자
- Scopus EID
- 2-s2.0-85163285323
- WoS UID
- 001141499900001



로그인
연구물 목록으로