Effect of substrate preheating on the microstructure and bending behavior of WC-Inconel 718 composite coating synthesized via laser directed energy deposition
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 피인용
- Web of Science 30Scopus 28
- FWCI (Scopus)
- 1.89
- JCR IF
- JCR 2022 3.6
- ISSN
- 0263-4368
저자
- 허 산산제1저자Pusan Natl Univ, Grad Sch Mech Engn, Busandaehak ro 63beon gil, Busan 46241, South Korea
- 박상후교신저자Pusan Natl Univ, Grad Sch Mech Engn, Busandaehak ro 63beon gil, Busan 46241, South Korea
- Shim, Do-sik교신저자Korea Maritime & Ocean Univ, Dept Ocean Adv Mat Convergence Engn, 727 Taejong ro, Busan 49112, South Korea
- Yao, ChangliangKorea Maritime & Ocean Univ, Dept Ocean Adv Mat Convergence Engn, 727 Taejong ro, Busan 49112, South Korea
- Li, MingchuanHarbin Inst Technol, State Key Lab Adv Welding & Joining, Harbin 150001, Peoples R China
- Wang, ShuanglongMax Planck Inst Polymer Res, Ackermannweg 10, D-55128 Mainz, Germany
초록
In this study, a substrate is reinforced with WC/Inconel 718 composite coating via directed energy deposition (DED). During the DED, the substrate was preheated to 300 °C and 500 °C. The microstructural characteristics of the matrix, fusion area, and area around the WC particles were systematically investigated. The results showed that the depth of the transition zone at the interface of the deposited layer and substrate for preheating to 500 °C increased, enhancing the metallurgical bonding between the deposited layer and the substrate. Additionally, three different types of WC particle diffusion mechanisms were exhibited: (i) slight dissolution diffusion for non-preheating sample, (ii) dissolution-diffusion fragmentation for 300 °C-preheating sample, and (iii) disintegration and diffusion for 500 °C-preheating sample. In contrast, the effects of dispersion and solid solution strengthening are more pronounced than that of the microstructure coarsening caused by preheating, resulting in a higher hardness value of 384.0 HV0.1 (preheating at 300 °C) and 381.3 HV0.1 (preheating at 500 °C) compared to that of the non-preheated sample (358.9 HV0.1). Furthermore, the bending fracture of the WC/Inconel 718 composite layer exhibited typical pseudo-ductile behavior with premature fracture. Consequently, the highest bending strength occurred at preheating 500 °C, in which the maximum bending load and the displacement at the initial crack increased by 9.15% and 39.69%, respectively, compared with the non-preheated sample. Additionally, the fracture mechanism exhibited mainly intergranular fracture and less transgranular fracture.
키워드
Bending testDirected energy depositionSubstrate preheatingWCSTRENGTHALLOY