본문 바로가기

Enhanced Metal Coating Adhesion by Surface Modification of 3D Printed PEKKs

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q2Scopus Q2
저널
COATINGS12(6) · #854 · 2022
피인용
Web of Science 18Scopus 21
FWCI (Scopus)
1.06
JCR IF
JCR 2021 3.236
ISSN
2079-6412

저자

  1. 백인우제1저자Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
  2. Lim, Chul-MinAgcy Def Dev, Def Space Technol Ctr, Daejeon 34186, South Korea
  3. Park, Kyoung YoulAgcy Def Dev, Def Space Technol Ctr, Daejeon 34186, South Korea
  4. 류봉기교신저자Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea

초록

PEKK (polyether-ketone-ketone) polymer has been actively studied in applying electronic devices in satellites owing to its excellent light weight and thermal resistance. However, the limitation of metal coating to form on the PEKK surface is due to the high-volume resistivity and surface resistance. Here, we have investigated the correlations between the chemical treatment of the surface and adhesion strength between polymer-metal coating. Three-dimensional printed PEKK objects were manufactured and nickel was deposited on the surface by electroless plating. As the concentration of H2SO4 increased from 12.5 to 14.3 mol/L, the pore diameter showed a tendency to increase. However, as growing pore induced connecting each other, the pore size re-decreased from 15.1 to 18.0 mol/L. To control pore size and uniformity, we investigated the pore diameter of 3D printed PEKK as a function of treatment time and temperature. Uniform pores were observed at a temperature of 50 degrees C which were formed after 10 min and the average pore size was 0.28 mu m. After H2SO4 swelling, samples were re-treated in the KMnO4-H3PO4 etching system for the hydrophilic group. KMnO4 broken C=C bonding and generated hydrophilic groups such as -COOH and -OH, the contact angle decreased from 64.7 to 51.1 degrees compared with H2SO4 swelling. XPS survey spectra confirmed that not only breaking C=C bonding but also increasing hydrophilicity due to -OH, -C-, -SO3 and the catalyst absorption of Pd was improved. As a result of adhesive strength by ASTM D3359, compared with the H2SO4 swelling, the KMnO4-H3PO4 etching system showed 5B which is the best result in standard test methods by adhesive tape test and peeling amount on the tape was less than 0.01%.

키워드

super engineering plasticpolyether-ketone-ketone3D printingelectroless platingadhesion forceELECTROLESS COPPERABS RESINPRETREATMENTIMPROVEMENT