Shape Recovery and Mechanical Properties of Hot-Rolled Fe–17Mn–5Si–5Cr–4Ni–0.1C–0.2Ti Shape Memory Alloy for Linear Actuator Application
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q3Scopus Q3
- 저널
- PHYSICS OF METALS AND METALLOGRAPHY123(14) · pp.1461 · 2022
- 피인용
- Web of Science 1Scopus 1
- FWCI (Scopus)
- 0.08
- JCR IF
- JCR 2021 1.319
- ISSN
- 0031-918X
저자
- 김도형제1저자Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- Hong, KinamChungbuk Natl Univ, Dept Civil Engn, Chungju 28644, South Korea
- Lee, JeonghoonPukyong Natl Univ, Dept Met Engn, Busan 48513, South Korea
- 이욱진교신저자Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
- 박용호Pusan Natl Univ, Sch Mat Sci & Engn, Busan 46241, South Korea
초록
Abstract: In this study, the relationship between the alloying element, microstructure, shape memory, and mechanical properties of a hot-rolled Fe–17Mn–5Si–5Cr–4Ni–0.2Ti–0.1C (wt %) alloy was investigated. In as-rolled state, the sample showed a high shape memory effect (SME) of ~3.06, 0.2% proof yield strength of 443 MPa, and a tensile strength of 1016 MPa. This is explained by the formation of TiC precipitates and stacking faults, as well as the thin ɛ phase. The SME, 0.2% proof yield, and tensile strength of the sample heat-treated at 600°C were 3.46%, 456, and 999 MPa, respectively. The improved SME was attributable to the slightly recovered temperature in this temperature range, whereas changes in the TiC precipitate distribution had no influence on the SME. Heat treatment at a higher temperature, however, drastically decreased both the SME and strength. This was mainly attributed to the recrystallization and the high density of the thick ɛ phase.
키워드
Fe–Mn–Simechanical propertiesmicrostructureshape memory alloyCIVIL ENGINEERING STRUCTURESTIC PRECIPITATIONTRANSFORMATIONBEHAVIORDEFORMATIONNBC