Temperature-Dependent Hydrogen Embrittlement of Austenitic Stainless Steel on Phase Transformation
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q1
- 저널
- METALS13(1) · 2023
- 피인용
- Web of Science 16Scopus 22
- FWCI (Scopus)
- 1.43
- JCR IF
- JCR 2022 2.9
- ISSN
- 2075-4701
저자
- 최영환제1저자Pusan Natl Univ, Dept Naval Architecture & Ocean Engn, Busan 46241, South Korea
- Lee, Jung HeeKorea Res Inst Ships & Ocean Engn KRISO, Offshore Ind R&BD Ctr, Geoje Si 53201, South Korea
- 김석민Pusan Natl Univ, Dept Naval Architecture & Ocean Engn, Busan 46241, South Korea
- 이동하Pusan Natl Univ, Dept Naval Architecture & Ocean Engn, Busan 46241, South Korea
- 김희태Pusan Natl Univ, Dept Naval Architecture & Ocean Engn, Busan 46241, South Korea
- 김정현Pusan Natl Univ, Hydrogen Ship Technol Ctr, Busan 46241, South Korea
- 김민정Pusan Natl Univ, Hydrogen Ship Technol Ctr, Busan 46241, South Korea
- 김슬기교신저자Pusan Natl Univ, Hydrogen Ship Technol Ctr, Busan 46241, South Korea
- 이제명교신저자Pusan Natl Univ, Dept Naval Architecture & Ocean Engn, Busan 46241, South Korea
초록
© 2022 by the authors.A critical issue that needs to be addressed for wider utilization of hydrogen as fuel is protection against hydrogen embrittlement during cryogenic storage as it weakens the microstructure bonding force of metals through hydrogen penetration. Austenitic stainless steel, which is usually used in cryogenic vessels and is well known for its high hydrogen resistance at room temperature, has also been reported to be vulnerable to hydrogen embrittlement under cryogenic temperatures. In addition, because large storage vessels are operated over a wide range of temperatures, material behavior at various temperature conditions should also be considered. Therefore, in the present study, hydrogen charging of austenitic stainless steel was performed under various temperature conditions for carrying out prestrain and tensile tests. A decrease in the tensile strength and elongation and an increase in the yield strength were observed in all cases. In particular, the case of 20% prestrain at cryogenic temperature followed by tensile test at room temperature after hydrogen charging showed fracture in the elastic region. The hydrogen index was evaluated from the perspective of elongation and reduction in area, which are factors that indicate the degree of ductility. The aforementioned case showed the most severe results, while non-prestraining followed by tensile tests at room temperature was the least effected by hydrogen. In addition, the effect of strain-induced martensite on hydrogen embrittlement was analyzed using electron backscattered diffraction (EBSD). It was observed that the higher is the prestrain at cryogenic temperatures, the greater is the volume fraction of α’ martensite, which leads to hydrogen embrittlement. The edges and center of the fracture surface were analyzed using scanning electron microscopy (SEM). The hydrogen-charged specimens exhibited brittle fractures at the edges and ductile fractures at the center. The more severe the embrittlement, the more were the number of intergranular fractures and microdimples observed at the edges.
키워드
hydrogen embrittlementhydrogen indexliquid-hydrogen storageprestrain effecttransformation-induced plasticityINDUCED MARTENSITE-TRANSFORMATIONMECHANICAL-PROPERTIESSTRAIN-RATEDEFORMATIONTENSILEENVIRONMENTPRESTRAINFRACTUREFAILURE