Soft magnetic composites with improved heat resistance and mechanical strength realized using Fe@SiO2 powders with a variable thickness insulation layer
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q1
- 저널
- JOURNAL OF MATERIALS SCIENCE57(38) · pp.18118 · 2022
- 피인용
- Web of Science 19Scopus 20
- FWCI (Scopus)
- 1.05
- JCR IF
- JCR 2021 4.682
- ISSN
- 0022-2461
저자
- Jang, Min-Sun제1저자Korea Inst Mat Sci KIMS, Met Powder Dept, 797 Changwondae Ro, Chang Won 51508, South Korea
- 박종민Pusan Natl Univ, Sch Mat Sci & Engn, Busandaehak Ro 63Beon Gil, Busan 46241, South Korea
- Kang, JinhoSungkyunkwan Univ SKKU, Dept Mat Sci & Engn, Suwon 16419, South Korea
- Sun, ChanghyoSungkyunkwan Univ SKKU, Dept Mat Sci & Engn, Suwon 16419, South Korea
- 구본욱Pusan Natl Univ, Sch Mat Sci & Engn, Busandaehak Ro 63Beon Gil, Busan 46241, South Korea
- Kim, Hea-RanKorea Inst Mat Sci KIMS, Met Powder Dept, 797 Changwondae Ro, Chang Won 51508, South Korea
- Kwon, Young-TaeKorea Inst Mat Sci KIMS, Met Powder Dept, 797 Changwondae Ro, Chang Won 51508, South Korea
- Yang, SangsunKorea Inst Mat Sci KIMS, Met Powder Dept, 797 Changwondae Ro, Chang Won 51508, South Korea
- Kim, YunseokSungkyunkwan Univ SKKU, Dept Mat Sci & Engn, Suwon 16419, South Korea
- Jeong, Jae Won교신저자Korea Inst Mat Sci KIMS, Met Powder Dept, 797 Changwondae Ro, Chang Won 51508, South Korea
초록
Here, we demonstrate a novel Fe@SiO2-powder-based soft magnetic composite that can withstand high-temperature heat treatment and that exhibits unprecedented mechanical strength. Fe@SiO2 powders are prepared by forming a uniform and continuous SiO2 insulation layer on the surface of Fe powder through sol-gel method based on a hydrolysis and condensation reaction mechanism. The sol-gel kinetics responded with a different tetraethyl orthosilicate (TEOS) concentration in the solution from 0.01 to 0.25 ml/g; SiO2 reactant is produced at different rates and accumulates at different thicknesses on the surfaces of Fe powders. The SMC core with dense and uniform SiO2 insulating layer contributes to better magnetic performance, including much higher electrical resistance, lower eddy current loss, and better frequency stability compared to those characteristics of the conductive Fe-based powder core. Furthermore, Fe@SiO2 SMC maintains its internal insulation matrix and low core loss even after high-temperature heat treatment, which densifies the SiO2 insulation layer and greatly enhances the mechanical strength of the SMCs. As a result, the Fe@SiO2 SMC core with an optimally controlled insulation thickness not only demonstrated a remarkably low core loss of 98 W/kg at 1 kHz and 500 mT but also a high mechanical flexural strength of 82 MPa, attributable to the uniform and dense internal SiO2 insulating matrix with high-temperature annealing resistance.