Digital Wear Analysis of Different CAD/CAM-Fabricated Monolithic Ceramic Implant-Supported Single Crowns Using Two Optical Scanners
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q4Scopus Q2
- 저널
- INTERNATIONAL JOURNAL OF PROSTHODONTICS35(3) · pp.357 · 2022
- 피인용
- Web of Science 11Scopus 12
- FWCI (Scopus)
- 1.58
- JCR IF
- JCR 2021 1.785
- ISSN
- 0893-2174
저자
- Marchand, Laurent제1저자교신저자Univ Geneva, Univ Clin Dent Med, Div Fixed Prosthodont & Biomat, Geneva, Switzerland
- Sailer, IrenaUniv Geneva, Univ Clin Dent Med, Div Fixed Prosthodont & Biomat, Geneva, Switzerland
- 이현종Pusan Natl Univ, Sch Dent, Dent Res Inst, Dept Prosthodont, Yangsan, South Korea
- Mojon, PhilippeUniv Geneva, Univ Clin Dent Med, Div Fixed Prosthodont & Biomat, Geneva, Switzerland
- Pitta, JoaoUniv Geneva, Univ Clin Dent Med, Div Fixed Prosthodont & Biomat, Geneva, Switzerland
초록
Purpose: To digitally evaluate the volumetric wear of four different implant crown materials and their antagonists after artificial aging using an intraoral scanner (IOS) device and a laboratory desktop scanner. Materials and Methods: A total of 48 implants were restored with monolithic crowns and divided into groups according to restorative material: lithium disilicate (LDS); zirconia (ZR); polymer-infiltrated ceramic network (PICN); and porcelain fused to metal (PFM). Each specimen was scanned using a desktop scanner (LAB group; iScan D104, (metric 3D) and an IOS device (IOS group; Trios 3, 3Shape) before and after chewing simulation (1,200,000 cycles, 49 N, steatite antagonist, 5 degrees C to 50 degrees C). The obtained STL files were superimposed, and the volumetric loss of substance of the crowns and their antagonists was quantified. Kruskal-Wallis, Spearman p, and paired t tests were used to analyze the data (alpha = .05). Results: The mean volume loss for each restorative material varied between 0.05 +/- 0.06 mm(3) (ZR/IOS) and 3.42 +/- 1.65 mm(3) (LDS/LAB). The wear of the antagonists was significantly lower (P < .05) for ZR than the other groups. Increased wear of the crowns was highly correlated with increased wear of their antagonists (r(s) = 0.859). When comparing the wear measurement using the two scanning devices, no difference in mean volume loss was found (IOS: 1.81 +/- 1.81 mm(3); LAB: 1.82 +/- 1.78 mm(3)) (P = .596). Conclusion: Polished ZR was the most wear-resistant material and the least abrasive to the respective antagonist among the tested ceramics. For quantification of wear, this IOS device can be used as an alternative to desktop scanners.
키워드
IN-VITRO WEAR2-BODY WEARTOOTH WEARDENTAL CERAMICSCOMPOSITE RESINENAMEL WEAREXAMINATION BEWEGLAZED ZIRCONIAPERFORMANCEANTAGONIST
식별자
- Scopus EID
- 2-s2.0-85132455835
- WoS UID
- 000817913600012



로그인
연구물 목록으로