Effect of Corrugated Sheet Diameter on Structural Behavior under Cryogenic Temperature and Hydrodynamic Load
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q1
- 저널
- METALS12(3) · 2022
- 피인용
- Web of Science 8Scopus 9
- FWCI (Scopus)
- 0.51
- JCR IF
- JCR 2021 2.695
- ISSN
- 2075-4701
저자
- 박진석제1저자Pusan Natl Univ, Dept Naval Architecture & Ocean Engn, Busan 46241, South Korea
- 김정현교신저자Pusan Natl Univ, Hydrogen Ship Technol Ctr, Busan 46241, South Korea
- 정용철Pusan Natl Univ, Dept Naval Architecture & Ocean Engn, Busan 46241, South Korea
- 김희태Pusan Natl Univ, Dept Naval Architecture & Ocean Engn, Busan 46241, South Korea
- 김슬기Pusan Natl Univ, Hydrogen Ship Technol Ctr, Busan 46241, South Korea
- 이제명교신저자Pusan Natl Univ, Dept Naval Architecture & Ocean Engn, Busan 46241, South Korea
초록
© 2022 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https:// creativecommons.org/licenses/by/ 4.0/).The most important technical issue in the shipbuilding industry regarding liquefied natural gas (LNG) carrier cargo containment systems (CCS) is securing the structural reliability of the primary barrier, which is in direct contact with the LNG. Fracture of the primary barrier by the hydrodynamic load of the LNG CCS may lead to disasters because it is difficult to implement immediate safety measures in the marine environment, unlike on land. Hence, structural reliability of the LNG membrane is the most critical issue in LNG carrier CCSs, where thin and corrugated 304L stainless steel is often used as the primary barrier to prevent repeated thermal deformation from the temperature difference during loading (−163◦C) and unloading (20◦C) of the LNG. However, plastic deformation of the 1.2 mm-thick corrugated membrane of the LNG CCS has been reported continuously owing to its vulnerability to cryogenic hydrodynamic loads. In the present study, we conducted a parametric analysis to investigate the effects of the corrugation shape as a preliminary study of the primary barrier. Finite element analysis was conducted with a simplified plate to focus on the effects of corrugation. Furthermore, a two-step validation was conducted using the above experimental results to ensure reliability of the structural analysis. The results show that optimizing the corrugation shape could ensure better structural safety than the conventional design.
키워드
CryogenicFinite element analysisLNG cargo containment systemLow-temperature stainless steel plateMetallic corrugated plateAUSTENITIC STAINLESS-STEELVISCOPLASTIC DAMAGE MODELMECHANICAL-PROPERTIESLNGDEFORMATIONRESISTANCEDESIGN
식별자
- Scopus EID
- 2-s2.0-85126771813
- WoS UID
- 000774104800001



로그인
연구물 목록으로