본문 바로가기

Multiscale simulation approach to investigate the binder distribution in catalyst layers of high-temperature polymer electrolyte membrane fuel cells

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q2Scopus Q1
저널
SCIENTIFIC REPORTS12(1) · 2022
피인용
Web of Science 11Scopus 11
FWCI (Scopus)
0.28
JCR IF
JCR 2021 4.997
ISSN
2045-2322

저자

  1. 권성현제1저자Pusan Natl Univ, Sch Chem Engn, 2,Busandaehak Ro 63Beon Gil, Busan 46241, South Korea
  2. Lee, So YoungKorea Inst Sci & Technol, Hydrogen & Fuel Cell Res Ctr, Hwarang Ro 14 Gil 5, Seoul 02792, South Korea
  3. Kim, Hyoung-JuhnKorea Inst Sci & Technol, Hydrogen & Fuel Cell Res Ctr, Hwarang Ro 14 Gil 5, Seoul 02792, South Korea
  4. Yim, Sung-DaeKorea Inst Energy Res KIER, Fuel Cell Lab, Daejeon 34129, South Korea
  5. Sohn, Young-JunKorea Inst Energy Res KIER, Fuel Cell Lab, Daejeon 34129, South Korea
  6. 이승걸교신저자Pusan Natl Univ, Sch Chem Engn, 2,Busandaehak Ro 63Beon Gil, Busan 46241, South Korea

초록

© 2022, The Author(s).A multiscale approach involving both density functional theory (DFT) and molecular dynamics (MD) simulations was used to deduce an appropriate binder for Pt/C in the catalyst layers of high-temperature polymer electrolyte membrane fuel cells. The DFT calculations showed that the sulfonic acid (SO3−) group has higher adsorption energy than the other functional groups of the binders, as indicated by its normalized adsorption area on Pt (− 0.1078 eV/Å2) and carbon (− 0.0608 eV/Å2) surfaces. Consequently, MD simulations were performed with Nafion binders as well as polytetrafluoroethylene (PTFE) binders at binder contents ranging from 14.2 to 25.0 wt% on a Pt/C model with H3PO4 at room temperature (298.15 K) and operating temperature (433.15 K). The pair correlation function analysis showed that the intensity of phosphorus atoms in phosphoric acid around Pt (ρPgPt - P(r)) increased with increasing temperature because of the greater mobility and miscibility of H3PO4 at 433.15 K than at 298.15 K. The coordination numbers (CNs) of Pt–P(H3PO4) gradually decreased with increasing ratio of the Nafion binders until the Nafion binder ratio reached 50%, indicating that the adsorption of H3PO4 onto the Pt surface decreased because of the high adsorption energy of SO3− groups with Pt. However, the CNs of Pt–P(H3PO4) gradually increased when the Nafion binder ratio was greater than 50% because excess Nafion binder agglomerated with itself via its SO3− groups. Surface coverage analysis showed that the carbon surface coverage by H3PO4 decreased as the overall binder content was increased to 20.0 wt% at both 298.15 and 433.15 K. The Pt surface coverage by H3PO4 at 433.15 K reached its lowest value when the PTFE and Nafion binders were present in equal ratios and at an overall binder content of 25.0 wt%. At the Pt (lower part) surface covered by H3PO4 at 433.15 K, an overall binder content of at least 20.0 wt% and equal proportions of PTFE and Nafion binder are needed to minimize H3PO4 contact with the Pt.