Fracture behaviors at inclusions of very-high-cycle fatigue in newly developed clean bearing steel
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q3Scopus Q3
- 저널
- INTERNATIONAL JOURNAL OF MODERN PHYSICS B35(26) · 2021
- 피인용
- Web of Science 11Scopus 10
- FWCI (Scopus)
- 0.82
- JCR IF
- JCR 2020 1.219
- ISSN
- 0217-9792
저자
- Suh, Min-Soo제1저자Korea Institute of Energy Research, Daejeon 34129, Republic of Korea
- Nahm, Seung-HoonKorea Research Institute of Standards and Science, Daejeon 34113, Republic of Korea
- Suh, Chang-Min교신저자School of Mechanical Engineering, Kyungpook National University, Daegu Campus, Daegu 41566, Republic of Korea
- 이슬비School of Materials Science and Engineering, Pusan National University, Busan Campus, Busan 46241, Republic of Korea
초록
© 2021 World Scientific Publishing Company.Bearing steel is essential for the driving parts of the rotating body, but fisheye crack of inclusions such as TiN, Al2O3 and Cr matrix is formed in the very-high-cycle fatigue (VHCF) regime. Therefore, research on the development of a clean bearing steel that reduces the size of inclusion such as TiN or that does not contain inclusion has been made recently. In this study, the results of long-term attempts by the maker to improve the performance and quality of bearing steel for very long life were quantitatively analyzed from the viewpoint of fracture mechanics. In other words, the phase transformation properties, VHCF characteristics with ultrasonic nanocrystal surface modification (UNSM) treatment and fracture mechanics analysis of this clean bearing are compared quantitatively with those of other common bearing steels from the viewpoint of engineering and industrial applications. The quenching and tempering (QT) specimens of the clean bearing showed fisheye cracks and duplex S-N curves in the VHCF regime. The fisheye crack of the clean bearing steel was an internal fatigue crack caused by a small inclusion mainly composed of Al2O3 in the VHCF region. However, fisheye cracking due to TiN and Cr matrix, which was observed in other common bearing steels, did not occur in the clean bearing steel due to the efforts of the developers of new clean bearing.
키워드
bearing steelduplex S - N curvesFisheye crackinclusionultrasonic nanocrystal surface modificationvery high cycle fatigue