본문 바로가기

Vickers crack extension and residual fracture strength of annealed and thermally tempered glass in water

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q1Scopus Q1
저널
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY42(4) · pp.1743 · 2022
피인용
Web of Science 9Scopus 10
FWCI (Scopus)
0.41
JCR IF
JCR 2021 6.364
ISSN
0955-2219

저자

  1. 김홍석제1저자Pusan Natl Univ, Grad Sch Mech Engn, Busan 46241, South Korea
  2. 박상후교신저자Pusan Natl Univ, Grad Sch Mech Engn, Busan 46241, South Korea

초록

© 2021 Elsevier LtdThe effect of water contact on the propagation of microscale surface cracks is investigated in two types of glass: annealed and tempered glass. Initial flaw is artificially created on the glass surface using a Vickers indenter, and is covered with a water droplet for 20 min. Micrographs of the flaw taken before and after water contact confirms the increase in crack length from around 61–103 μm for thermally tempered glass. After water dipping, the maximum length to which the crack growth is approximately 57 % smaller in the thermally tempered glass than in the annealed glass. Despite the severe effect of water contact on crack propagation, it is found that the fracture strength is not substantially altered by water dipping; even though the crack length is enlarged, the fracture strength of glass is similar, and in the case of tempered glass, its fracture strength is slightly changed within 7% due to the blunting of the crack tip by water or others.

키워드

Annealed glassCrack growthFracture strengthSi-O dissolutionThermally tempered glass

식별자

Scopus EID
2-s2.0-85120772510
WoS UID
000742858000003