Development and Characteristics of Aerated Alkali-Activated Slag Cement Mixed with Zinc Powder
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q2
- 저널
- MATERIALS14(21) · #6293 · 2021
- 피인용
- Web of Science 9Scopus 9
- FWCI (Scopus)
- 0.49
- JCR IF
- JCR 2020 3.623
- ISSN
- 1996-1944
저자
- 김태완제1저자Pusan Natl Univ, Dept Civil Engn, Busan 46241, South Korea
- Kang, Choonghyun교신저자Gyeongsang Natl Univ, Dept Ocean Civil Engn, Tongyeong 53064, South Korea
- Seo, KiyoungHK Engn & Consultants, Busan 46220, South Korea
초록
Experiments on the development and properties of aerated concrete based on alkali-activated slag cement (AASC) and using Zn powder (ZP) as a gas agent were carried out. The experiments were designed for water-binding material (w/b) ratios of 0.35 and 0.45, curing temperatures of 23 & PLUSMN; 2 & DEG;C and 40 & PLUSMN; 2 & DEG;C, and ZP of 0.25%, 0.50%, 0.75%, and 1.0%. ZP generates hydrogen (H-2) gas in AASC to form pores. At a w/b of 0.35, the curing temperature had little effect on the pore size by ZP. However, a w/b of 0.45 showed a clear correlation that the pore diameter increased as the curing temperature increased. The low w/b of 0.35 showed a small change in the pore size according to the curing temperature due to the faster setting time than 0.45 and the increased viscosity of the paste. Therefore, at a termination time exceeding at least 60 min and a w/b of 0.45 or more, it was possible to increase the size and expansion force of the pores formed by the ZP through the change of the curing temperature. ZP showed applicability to the manufacture of AASC-based aerated concrete, and the characteristics of foaming according to the curing temperature, w/b ratio, and ZP concentration were confirmed.
키워드
zinc powdergas agentalkali-activated slag cementhydrogen gasaerated concreteFOAMING AGENTZNONANOPARTICLESALUMINUM
식별자
- Scopus EID
- 2-s2.0-85117851808
- WoS UID
- 000719034800001