Torsional Resistance of Heat-Treated Nickel-Titanium Instruments under Different Temperature Conditions
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q2
- 저널
- MATERIALS14(18) · #5295 · 2021
- 피인용
- Web of Science 9Scopus 12
- FWCI (Scopus)
- 0.49
- JCR IF
- JCR 2020 3.623
- ISSN
- 1996-1944
저자
- Jo, Hyo Jin제1저자Kyungpook Natl Univ, Sch Dent, Dept Conservat Dent, Daegu 41940, South Korea
- 곽상원Pusan Natl Univ, Sch Dent, Dent Res Inst, Dept Conservat Dent, Yangsan 50612, South Korea
- 김현철Pusan Natl Univ, Sch Dent, Dent Res Inst, Dept Conservat Dent, Yangsan 50612, South Korea
- Kim, Sung KyoKyungpook Natl Univ, Sch Dent, Dept Conservat Dent, Daegu 41940, South Korea
- Ha, Jung-Hong교신저자Kyungpook Natl Univ, Sch Dent, Dept Conservat Dent, Daegu 41940, South Korea
초록
This study compared the torsional resistance of heat-treated nickel-titanium (NiTi) instruments under different temperature conditions. Four thermomechanically treated single-use NiTi rotary instruments were selected for this study: OneShape (OS), OneCurve (OC), WaveOne Gold (WOG) and HyFlex EDM (HFE). Each instrument was further subdivided by temperature into 2 subgroups. Maximum torque and the distortion angle until fracture occurred were evaluated. Differential scanning calorimetry analysis was performed to measure the phase transformation temperature. Statistical analysis was performed using a two-way ANOVA and t-test (p < 0.05). Fractured fragments were observed using scanning electron microscopy (SEM). The two-way ANOVA showed no significant differences for different temperature conditions. At both room (RT) and body temperature (BT), OS was predominantly austenite while HFE was martensite. OC and WOG were predominantly martensite at RT and mixed phase at BT. At BT, more than half of WOG was martensite, while half of OC was austenite. SEM examination showed no topographical differences between instruments in different temperature groups. In relation to a limitation of this study, there was no difference in torsional resistance of NiTi rotary instruments between the BT and RT conditions. This implies that clinicians do not need to consider a decrease of torsional resistance of heat-treated NiTi instruments at BT.
키워드
body temperatureC-wiredifferential scanning calorimetryelectrical discharge machininggold-wireheat-treated nickel-titanium filetorsional resistanceROTARY ENDODONTIC INSTRUMENTSPHASE-TRANSFORMATION BEHAVIORCYCLIC FATIGUEMECHANICAL-PROPERTIESSEM OBSERVATIONSFILES