Effects of solution treatment temperature and time on the porosities and mechanical properties of vacuum die-casted and T6 heat-treated Al-Si-Mg alloy
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q1
- 저널
- VACUUM193 · #110536 · 2021
- 피인용
- Web of Science 61Scopus 67
- FWCI (Scopus)
- 3.13
- JCR IF
- JCR 2020 3.627
- ISSN
- 0042-207X
저자
- 강호정제1저자Pusan Natl Univ, Dept Mat Sci & Engn, Busan 609735, South Korea
- 장호성Pusan Natl Univ, Dept Mat Sci & Engn, Busan 609735, South Korea
- 오성효Pusan Natl Univ, Dept Mat Sci & Engn, Busan 609735, South Korea
- Yoon, Pil-hwanKorea Inst Ind Technol, Adv Forming Proc R&D Grp, Ulsan 44776, South Korea
- Lee, Gyu-heunKorea Inst Ind Technol, Adv Forming Proc R&D Grp, Ulsan 44776, South Korea
- Park, Jin-youngKorea Inst Ind Technol, Adv Forming Proc R&D Grp, Ulsan 44776, South Korea
- Kim, Eok-soo교신저자Dongnam Precis Co Ltd, Ulsan 44776, South Korea
- 최윤석교신저자Pusan Natl Univ, Dept Mat Sci & Engn, Busan 609735, South Korea
초록
Al-Si-Mg cast alloys can be imparted with a wide range of mechanical properties through heat treatment, thus meeting the required performance of various vehicle components. However, because of the characteristics of the high-pressure die casting process, the gas porosities in the casting can lead to blisters during the solution treatment of die-casting parts. Therefore, systematic studies on the solution temperature and solution time are required to prevent such blisters. In this study, the gas porosity and mechanical properties of T6 heat-treated specimens were evaluated under various solution treatment conditions. As the solution treatment temperature and time increased, the numbers and volume of individual gas porosity increased. On the other hand, there were little changes in the shrinkages upon heat treatment. As solution temperature and time increased, the area fraction of the eutectic Si particles and Mg2Si decreased slightly, whereas the area and sphericity of the eutectic Si and Mg2Si increased. As the solution treatment temperature and time increased, the ultimate tensile strength and yield strength increased, whereas the elongation tended to decrease. However, the maximum UTS and YS were obtained on treatment at 520 degrees C for 1.5 h.
키워드
Vacuum die castingAl-Si-Mg alloySolution treatment temperatureSolution treatment timePorosityALUMINUM BIPOLAR PLATESMICROSTRUCTUREBEHAVIORCUBLISTERFABRICATIONDUCTILITY
식별자
- Scopus EID
- 2-s2.0-85113306165
- WoS UID
- 000702762500005



로그인
연구물 목록으로