Hydrogen-rich gas production via steam gasification of food waste over basic oxides (MgO/CaO/SrO) promoted-Ni/Al2O3 catalysts
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- CHEMOSPHERE287 · #132224 · 2022
- 피인용
- Web of Science 36Scopus 38
- FWCI (Scopus)
- 1.6
- JCR IF
- JCR 2021 8.943
- ISSN
- 0045-6535
저자
- Moogi, Surendar제1저자Univ Seoul, Sch Environm Engn, Seoul 02504, South Korea
- 장성호Pusan Natl Univ, Dept Bioenvironm Energy, Miryang 50463, South Korea
- Rhee, Gwang HoonUniv Seoul, Dept Mech & Informat Engn, Seoul 02504, South Korea
- Ko, Chang HyunChonnam Natl Univ, Sch Chem Engn, Gwangju 61186, South Korea
- Choi, Yong JunUniv Seoul, Sch Environm Engn, Seoul 02504, South Korea
- Lee, See HoonJeonbuk Natl Univ, Dept Mineral Resource & Energy Engn, Jeonju 54896, South Korea
- Show, Pau LokeUniv Nottingham Malaysia, Fac Sci & Engn, Dept Chem & Environm Engn, Jalan Broga, Semenyih 43500, Selangor Darul, Malaysia
- Lin, Kun-Yi AndrewNatl Chung Hsing Univ, Dept Environm Engn, 250 Kuo Kuang Rd, Taichung, Taiwan
- Park, Young-Kwon교신저자Univ Seoul, Sch Environm Engn, Seoul 02504, South Korea
초록
Food waste, a renewable resource, was converted to H-2-rich gas via a catalytic steam gasification process. The effects of basic oxides (MgO, CaO, and SrO) with 10 wt% Ni/Al2O3 on the gasification properties of food waste were investigated using a U-shaped gasifier. All catalysts prepared by the precipitation method were analyzed by X-ray diffraction, H-2-temperature-programmed reduction, NH3-temperature-programmed desorption, scanning electron microscopy, and energy-dispersive X-ray spectroscopy. The Ni/Al2O3 catalyst was reduced incompletely, and low nickel concentrations were detected on the surface of the alumina. The basic oxides minimized the number of acid sites and suppressed the formation of nickel-aluminate (NiAlxOy) phase in catalyst. In addition, the basic oxides shifted nickel-aluminate reduction reaction to lower temperatures. It resulted in enhancing nickel concentration on the catalyst surface and increasing gas yield and hydrogen selectivity. The low gas yield of the Ni/Al2O3 catalyst was attributed to the low nickel concentration on the surface. The maximum gas yield (66.0 wt%) and hydrogen selectivity (63.8 vol%) of the 10 wt% SrO-10 wt% Ni/Al2O3 catalyst correlated with the highly dispersed nickel on the surface and low acidity. Furthermore, coke deposition during steam gasification varied with the surface acidity of the catalysts and less coke was formed on 10 wt% SrO-10 wt% Ni/ Al2O3 due to efficient tar cracking. This study showed that the steam gasification efficiency of the Ni/Al2O3 catalyst could be improved significantly by the addition of SrO.
키워드
Food waste steam gasificationHydrogen-rich gasBasic oxides (MgO/CaO/SrO) promotionNi/Al2O3 catalystsSYNGAS PRODUCTIONNI CATALYSTSBIOMASSPYROLYSISGLYCEROLMETHANECAOMGOIMPREGNATIONPERFORMANCE
식별자
- Scopus EID
- 2-s2.0-85114692855
- WoS UID
- 000704968100001



로그인
연구물 목록으로