Consolidation and properties of tungsten by spark plasma sintering and hot isostatic pressing
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS99 · #105602 · 2021
- 피인용
- Web of Science 24Scopus 27
- FWCI (Scopus)
- 1.13
- JCR IF
- JCR 2020 3.871
- ISSN
- 0263-4368
저자
- Byun, Jong Min제1저자Seoul Natl Univ Sci & Technol, Dept Mat Sci & Engn, Seoul 01811, South Korea
- Lee, Eui SeonSeoul Natl Univ Sci & Technol, Dept Mat Sci & Engn, Seoul 01811, South Korea
- Heo, Youn JiSeoul Natl Univ Sci & Technol, Dept Mat Sci & Engn, Seoul 01811, South Korea
- 정영근Pusan Natl Univ, Grad Sch Convergence Sci, Busan 46241, South Korea
- Oh, Sung-Tag교신저자Seoul Natl Univ Sci & Technol, Dept Mat Sci & Engn, Seoul 01811, South Korea
초록
The fabrication of dense tungsten was attempted with the combination process of presintering by spark plasma sintering and final hot isostatic pressing. The specimens fabricated by spark plasma sintering (1500-1600 degrees C) of commercial powder exhibited a relative density above 90.4%. In the case of the post hot isostatic pressing at 1650 degrees C for 2 h, improved relative density in the range of 96.4% to 97.2% was obtained. X-ray diffractometry and X-ray photoelectron spectroscopy analysis indicated that the sintered specimen was composed mainly of tungsten, and the trace amounts of metallic tungsten are bound with oxygen due to the surface oxidation. Strength measurement was conducted by biaxial bending test using a piston-on-three balls. Maximum flexural strength of 761 MPa were obtained for tungsten consolidated by a combined process of spark plasma sintering and hot isostatic pressing. The strength increase is explained by the increase in relative density rather than the effect of particle size.
키워드
TungstenSpark plasma sinteringHot isostatic pressingMicrostructureFlexural strength