Effect of Postweld Heat Treatments on Type IV Creep Failure in the Intercritical Heat-Affected Zone of 10% Cr Martensitic Steel Welded with Haynes 282 Filler
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q2
- 저널
- METALS11(5) · 2021
- 피인용
- Web of Science 4Scopus 6
- FWCI (Scopus)
- 0.37
- JCR IF
- JCR 2020 2.351
- ISSN
- 2075-4701
저자
- 김남규제1저자Division of Materials Science and Engineering, Pusan National University, Busan, 46241, Korea
- Kang, YongjoonDepartment of Joining Technology, Korea Institute of Materials Science (KIMS), Changwon, 51508, Korea
- Bang, JinhyeokDepartment of Joining Technology, Korea Institute of Materials Science (KIMS), Changwon, 51508, Korea
- Song, SangwooDepartment of Joining Technology, Korea Institute of Materials Science (KIMS), Changwon, 51508, Korea
- Seo, Seong-MoonDepartment of High Temperature Materials, Korea Institute of Materials Science (KIMS), Changwon, 51508, Korea
- 강정윤교신저자Industrial Liaison Innovation Center, Pusan National University, Busan, 46241, Korea
- 강남현교신저자Division of Materials Science and Engineering, Pusan National University, Busan, 46241, Korea
초록
This study investigated the effect of postweld heat treatment (PWHT) conditions on Type IV failure behavior of 10% Cr martensitic steel welds using Haynes 282 filler. The welded joints were subjected to PWHT at temperatures of 688, 738, and 788 degrees C for 4 and 8 h. Creep tests were carried out at 600 degrees C under a stress of 200 MPa. The as-welded joint without PWHT showed Type IV cracking due to growth of voids around Laves phase by localized creep deformation in the intercritical heat-affected zone (ICHAZ). The creep properties of the PWHTed joints at 688 degrees C were similar to those of the as-welded joints without PWHT. On the other hand, the PWHTed joints at 738 degrees C exhibited a significantly longer creep life by a lower amount of Laves phase in the ICHAZ than those at 688 degrees C; this could be a result of the homogenization of ICHAZ microstructure during PWHT at 738 degrees C. However, the PWHT at 688 and 738 degrees C showed the same Type IV creep failure mode. Meanwhile, the PWHTed joints at 788 degrees C exhibited the shortest creep life in this study. The failure location was shifted to the base metal away from the HAZ, and severe plastic deformation occurred due to the softened matrix by excessive tempering.
키워드
postweld heat treatmentheat-affected zonecreep testType IV cracking10% Cr martensitic steelHIGH-TEMPERATURE TENSILELAVES PHASE PARTICLESMICROSTRUCTURE EVOLUTIONFERRITIC STEELPRECIPITATION BEHAVIORMECHANICAL-PROPERTIESCRACKING BEHAVIORDEFORMATIONSTRENGTHNUCLEATION
식별자
- Scopus EID
- 2-s2.0-85104884283
- WoS UID
- 000662579900001