Effect of Gas Bubbling Filtration Treatment Conditions on Melt Quality of AlSiMgCu Alloy
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q2
- 저널
- METALS11(5) · 2021
- 피인용
- Web of Science 8Scopus 8
- FWCI (Scopus)
- 0.37
- JCR IF
- JCR 2020 2.351
- ISSN
- 2075-4701
저자
- 장호성제1저자School of Materials Science and Engineering, Pusan National University, Busan, 46241, Korea
- 강호정School of Materials Science and Engineering, Pusan National University, Busan, 46241, Korea
- Lee, Gyu-HeunAdvanced Forming Process R&D Group, Korea Institute of Industrial Technology, Ulsan, 44776, Korea;
- Yoon, Pil-HwanAdvanced Forming Process R&D Group, Korea Institute of Industrial Technology, Ulsan, 44776, Korea;
- Park, Jin-YoungAdvanced Forming Process R&D Group, Korea Institute of Industrial Technology, Ulsan, 44776, Korea;
- 최윤석교신저자School of Materials Science and Engineering, Pusan National University, Busan, 46241, Korea
- Shin, Sunmi교신저자Advanced Forming Process R&D Group, Korea Institute of Industrial Technology, Ulsan, 44776, Korea;
초록
In this study, the optimal conditions of gas bubbling filtration (GBF) treatment for securing highly-clean molten Al-Si-Mg-Cu alloy were identified. The effects of GBF treatment time and stabilization time on the degree of molten metal cleanliness were examined by measuring melt quality parameters such as density index, bifilm index, porosity, and the amount of dissolved hydrogen [H]. A high melt quality was achieved when GBF treatment was performed on 10 kg melt for more than 10 min (i.e., 1 L gas/kg melt). However, as the stabilization holding time after GBF treatment increased to 10, 20, and 30 min, the melt quality degraded. GBF treatment for 30 min had a similar effect to treatment for 10 min, and the degree of deterioration of melt quality during the stabilization time was also similar. Considering the economics, 10 min GBF treatment and short holding time are required. Observations of the shape and volume of the largest pore suggested the cause of defect formation and confirmed that the volume of the largest pore can be used as an index of the melt quality.
키워드
reduced pressure testdensity indexbifilm indexporositydissolved hydrogenREDUCED PRESSURE TESTHYDROGEN SOLUBILITYMIXING TIMEALUMINUMREMOVAL