Phase control of WC-Co hardmetal using additive manufacturing technologies
- 문서 유형
- 연구출판물 · 리뷰논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q2
- 저널
- POWDER METALLURGY65(1) · pp.13 · 2022
- 피인용
- Web of Science 23Scopus 25
- FWCI (Scopus)
- 0.56
- JCR IF
- JCR 2021 2.228
- ISSN
- 0032-5899
저자
- Lee, Seung Woo제1저자Department of Metal Powder, Korea Institute of Materials Science, Changwon, Republic of Korea
- Kim, Yeon WooDepartment of Metal Powder, Korea Institute of Materials Science, Changwon, Republic of Korea
- Jang, Kyeong MiDepartment of Metal Powder, Korea Institute of Materials Science, Changwon, Republic of Korea
- 이진우School of Materials Science and Engineering, Pusan National University, Busan, Republic of Korea
- 박민수교신저자Department of Metal Powder, Korea Institute of Materials Science, Changwon, Republic of Korea
- Koo, Hye YoungDepartment of Metal Powder, Korea Institute of Materials Science, Changwon, Republic of Korea
- Ha, Gook-HyunDepartment of Metal Powder, Korea Institute of Materials Science, Changwon, Republic of Korea
- Kang, Yun ChanDepartment of Materials Science and Engineering, Korea University, Seoul, Republic of Korea
초록
Three-dimensional WC-Co hardmetal samples were fabricated using WC-Co nanopowder via two methods: selective laser melting (SLM) and fused deposition modelling (FDM). The carbon loss and phase transition during processing were controlled to minimise the degradation of mechanical properties of the cemented carbide. The SLM samples were manufactured from granule powder produced via spray drying, whereas the FDM process was carried out on a filament produced via injection moulding. During SLM, carbon loss occurred due to the high energy involved in the process. Owing to carbon loss, the relative density and Rockwell hardness of SLM processed samples were low. To overcome this, a stable WC phase cemented carbide was manufactured via FDM. The density of the sintered FDM samples was improved by increasing the packing density of the filaments. The carbide sintered samples had a relative density of 96.3%, hardness of HRA 89.06 and carbon content of 5.47-5.52 wt-%.
키워드
WC-Co hardmetaladditive manufacturingnanopowderselective laser meltingfused deposition modellingLASERPOWDER