본문 바로가기

Phase Formation and Wear Resistance of Carbon-Doped TiZrN Nanocomposite Coatings by Laser Carburization

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q2Scopus Q2
저널
METALS11(4) · 2021
피인용
Web of Science 8Scopus 8
FWCI (Scopus)
0.37
JCR IF
JCR 2020 2.351
ISSN
2075-4701

저자

  1. 김성훈제1저자School of Materials Science and Engineering, Pusan National University, Busan, 609-735, Korea
  2. 김태우School of Materials Science and Engineering, Pusan National University, Busan, 609-735, Korea
  3. 홍은표School of Materials Science and Engineering, Pusan National University, Busan, 609-735, Korea
  4. Jo, IlgukDivision of Advanced Materials Engineering, Dong-Eui University, Busan, 47340, Korea
  5. Kim, Jaeyoung교신저자College of Global Business, Korea University, 2511 Sejong-ro, Sejong City, 30019, Korea
  6. 이희수교신저자School of Materials Science and Engineering, Pusan National University, Busan, 609-735, Korea

초록

Carbon-doped TiZrN nanocomposite coatings were investigated for phase formation and wear behavior. They were prepared by laser carburization using carbon paste, and the thermal energy of the pulsed laser was limited to the range of 20 to 50%. X-ray photoelectron spectroscopy analysis revealed that the ratio of carbide (TiC, ZrC) increased as the thermal energy of the laser increased. The sp(2)/sp(3) ratio increased by approximately 16% when the laser thermal energy was raised from 30 to 40%, and the formation of amorphous carbon was confirmed in the carbon-doped TiZrN coatings. As a result of microstructural analysis, the carbon-doped TiZrN nanocomposite was formed by an increase of hybrid bonds in expanded localized carbon clusters. Wear resistance was evaluated using a ball-on-disc tester, which showed that the friction coefficient decreased from 0.74 to 0.11 and the wear rate decreased from 7.63 x 10(-6) mm(3) (Nm)(-1) to 1.26 x 10(-6) mm(3) (Nm)(-1). In particular, the friction coefficient and wear rate improved by 71 and 66%, respectively, owing to the formation of carbon-doped TiZrN nanocomposite with amorphous carbon while the thermal energy was increased from 30 to 40%.

키워드

laser carburizationcarbon-doped TiZrN nanocomposite coatingsamorphous carbonfriction coefficientwear rate