본문 바로가기

Mechanical Performance Degradation of Glass Fiber-reinforced Polyurethane Foam Subjected to Repetitive Low-energy Impact

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q1Scopus Q1
피인용
Web of Science 28Scopus 35
FWCI (Scopus)
1.32
JCR IF
JCR 2020 5.329
ISSN
0020-7403

저자

  1. 김명성제1저자Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, 46241, Republic of Korea
  2. 김정대Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, 46241, Republic of Korea
  3. 김정현Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, 46241, Republic of Korea
  4. 이제명교신저자Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, 46241, Republic of Korea

초록

Polyurethane foam (PUF) has excellent thermal insulation performance owing to its closed cellular solid structure. Additionally, this microstructural characteristic provides outstanding impact absorption performance. Owing to these advantages, PUF is widely adopted in transportation applications. From the viewpoint of use in practical applications, it is necessary to evaluate the residual strength after repetitive low-energy impacts on the structure. Thus, in the present study, we investigated the effects of repetitive low-energy impact on mechanical behavior of glass fiber-reinforced PUF. After the free-falling type repetitive impact test, a series of compressive tests were performed to investigate the effect of impact conditions on the compressive performance. As a result, the critical impact energy causing degradation of the impact and compressive performance of RPUF was 1,092 - 1,228 J/m(2). In the impact performance, the peak stress, impact duration, and peak strain decreased by 13.5%, increased by 28.5%, and increased by 35.2%, respectively, after 80 repetitions of a 1,500 J/m(2) impact. Moreover, under the same impact condition, the elastic modulus decreased by 44.5% compared to that of the intact specimen.

키워드

Glass fiber-reinforced polyurethane foamRepetitive impact loadingCompression after impactLow-energy impactPerformance degradation