오스테나이트계 경량철강의 냉각 조건에 따른 미세조직, 기계적 특성 이해 및 대형 슬라브 내부 특성 분포 예측 연구
Microstructures and mechanical properties of austenitic light-weight steels, and prediction of property distribution in large-scale slab
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q3Scopus Q2
- 저널
- Korean Journal of Metals and Materials58(12) · pp.830 · 2020
- 피인용
- Web of Science 4Scopus 4KCI 3
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2019 1.146
- ISSN
- 1738-8228
저자
- 김태하제1저자School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
- 최윤석교신저자School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
- Kim, Kyeong-WonDepartment of Steels, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- Park, Seong-Jun교신저자Department of Steels, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- Park, Jun YoungAuthorized Nuclear Inspection Department, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- Jeong, KyeongjaeDepartment of Materials Science and Engineering, Research Institute of Advanced Materials, Seoul National University, Seoul 08826, Republic of Korea
- Han, Heung NamDepartment of Materials Science and Engineering, Research Institute of Advanced Materials, Seoul National University, Seoul 08826, Republic of Korea
- Shin, Jong-HoCorporate Research and Development Institute, Doosan Heavy Industries and Construction Co. LTD, Changwon 51711, Republic of Korea
초록
The effects of the cooling rate, after solution heat treatment, on the microstructures and mechanical properties of Fe-22Mn-8Al-0.8C-0.02Nb (low carbon) and Fe-20Mn-8Al-1.1C-0.1Nb (high carbon) light-weight steels were systematically investigated. The cooling process was controlled to achieve six different cooling rates, ranging from -0.016 to -465.1 degrees C/s. Under the slowest cooling rate (furnace cooling), intra-granular and inter-granular precipitations of kappa-carbides were observed throughout the austenite grains. The higher the C content was, the larger the size of the inter-granular kappa-carbides was. The formation of kappa-carbides resulted in an increase in yield strength, and a decrease in elongation and impact absorbed energy. In the Fe-20Mn-8Al-1.1C-0.1Nb, the inter-granular precipitation of kappa-carbides caused a drastic decrease in the impact absorbed energy and the inter-granular brittle fracture. To predict the distribution of yield strength and impact absorbed energy at production scale (a 10-ton scale slab), finite element analysis was conducted for water cooling and air cooling conditions. The average cooling rates at the center of the slab under water cooling and air cooling were predicted to be -0.126 and -0.031 degrees C/s, respectively. Based on predicted cooling rates, the distribution of mechanical properties was determined. The prediction suggested that a large-scale slab of the light-weight steel with low C content would have good toughness at the center of the slab regardless of cooling condition.
키워드
light-weight steelcooling rate, kappa-carbidemechanical propertiesfinite element analysisMODULATED STRUCTUREINDUCED PLASTICITYFRACTURE-BEHAVIORMNCORROSIONALLOYTEMPERATUREMOSI