Dispersion Mechanism and Mechanical Properties of SiC Reinforcement in Aluminum Matrix Composite through Stir- and Die-Casting Processes
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q2
- 저널
- APPLIED SCIENCES-BASEL11(3) · 2021
- 피인용
- Web of Science 26Scopus 31
- FWCI (Scopus)
- 0.81
- JCR IF
- JCR 2020 2.679
- ISSN
- 2076-3417
저자
- 신상민제1저자Department of Functional Composites, Korea Institute of Materials Science (KIMS), Changwon, 51508, Korea
- Park, HyeonjaeDepartment of Functional Composites, Korea Institute of Materials Science (KIMS), Changwon, 51508, Korea
- Park, ByeongjinDepartment of Functional Composites, Korea Institute of Materials Science (KIMS), Changwon, 51508, Korea
- Lee, Sang-BokDepartment of Functional Composites, Korea Institute of Materials Science (KIMS), Changwon, 51508, Korea
- Lee, Sang-KwanDepartment of Functional Composites, Korea Institute of Materials Science (KIMS), Changwon, 51508, Korea
- 김양도School of Materials Science and Engineering, Pusan National University, Busan, 46241, Korea
- Cho, Seungchan교신저자Department of Functional Composites, Korea Institute of Materials Science (KIMS), Changwon, 51508, Korea
- Jo, Ilguk교신저자Department of Advanced Materials Engineering, Dong-Eui University, Busan, 47340, Korea
초록
In this study, different volume fractions of silicon-carbide-reinforced AA2024 matrix composites were successfully fabricated using stir-casting (SC) and die-casting (DC) processes. The microstructural difference and physical properties of the composites during the manufacturing process were investigated in detail. The microstructural analysis found that the composite produced by the SC process had some reinforcement clusters and pores; however, defects and clusters significantly decreased after the DC process. In particular, the degree of reinforcement dispersion was quantitatively analyzed and compared before and after the DC process using the dispersion-analysis method. As a result of quantitative evaluation, the degree of dispersion was improved 2.5, 4.6, and 4.0 times with 3 vol.%, 6 vol.%, and 9 vol.% SiC-reinforced composite after the DC process, respectively. The electron backscatter diffraction (EBSD) analysis showed that the grain size of the 9 vol.% SiC-reinforced DC composite (17.67 mu m) was 75% smaller than that of the SC composite (68.06 mu m). The average tensile strength and hardness of the 9 vol.% SiC-reinforced DC composite were 2 times higher than those of the AA2024 matrix. The superior mechanical properties of the DC-processed composite can be attributed to the increase in dispersivity of the SiC particles and to decreases in defects and grain size during the DC process.
키워드
Al matrix composites (AMCs)stir-casting (SC)die-casting (DC)dispersion mechanismmechanical properties