Effects of Substitution of Y with Yb and Ce on the Microstructures and Mechanical Properties of Mg88.5Zn5Y6.5
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q2
- 저널
- METALS11(1) · 2021
- 피인용
- Web of Science 2Scopus 3
- FWCI (Scopus)
- 0.15
- JCR IF
- JCR 2020 2.351
- ISSN
- 2075-4701
저자
- Liao, Hongxin제1저자College of Materials Science & Engineering, Chongqing University, Chongqing, 400044, China
- 이태경School of Mechanical Engineering, Pusan National University, Busan, 46241, Korea
- Song, JiangfengCollege of Materials Science & Engineering, Chongqing University, Chongqing, 400044, China
- Kim, Jonghyun교신저자College of Materials Science & Engineering, Chongqing University, Chongqing, 400044, China
- Pan, Fusheng교신저자College of Materials Science & Engineering, Chongqing University, Chongqing, 400044, China
초록
The microstructures and mechanical properties of the Mg88.5Zn5Y6.5-XREX (RE = Yb and Ce, X = 0, 1.5, 3.0, and 4.5) (wt.%) alloys were investigated in the present study. Mg88.5Zn5Y6.5 is composed of three phases, namely, alpha-Mg, long-period stacking ordered (LPSO) phases, and intermetallic compounds. The content of the LPSO phases decreased with the addition of Ce and Yb, and no LPSO phases were detected in Mg88.5Zn5Y2.0Yb4.5. The alloys containing the LPSO phases possessed a stratified microstructure and exhibited excellent mechanical properties. Mg88.5Zn5Y5.0Ce1.5 exhibited the highest creep resistance and mechanical strength at both room temperature and 200 degrees C, owing to its suitable microstructure and high thermal stability. The yield strength of Mg88.5Zn5Y5.0Ce1.5 at room temperature was 358 MPa. The ultimate tensile strength of Mg88.5Zn5Y5.0Ce1.5 at room temperature and 200 degrees C was 453 MPa and 360 MPa, respectively.
키워드
Mg-Zn-Y-RElong-period stacking ordered structuremechanical propertiescreep resistance