Metallic Niobium Powder Reduced by Atmospheric Magnesium Gas with Niobium Pentoxide Powder
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q3Scopus Q3
- 저널
- MATERIALS TRANSACTIONS62(1) · pp.34 · 2021
- 피인용
- Web of Science 7Scopus 7
- FWCI (Scopus)
- 0.37
- JCR IF
- JCR 2020 1.389
- ISSN
- 1345-9678
저자
- 박수진제1저자Department of Materials Science and Engineering, Pusan National University, 2, Busandaehak-ro 63 Beon-gil, Geumjeong-gu, Busan 46241, Korea
- 황선민Department of Materials Science and Engineering, Pusan National University, 2, Busandaehak-ro 63 Beon-gil, Geumjeong-gu, Busan 46241, Korea
- Wang, Jei-PilDepartment of Metallurgical Engineering, Pukyong National University, 45, Yongso-ro, Nam-gu, Busan 48513, Korea
- 손영국교신저자Department of Materials Science and Engineering, Pusan National University, 2, Busandaehak-ro 63 Beon-gil, Geumjeong-gu, Busan 46241, Korea
- Lee, Dong-Won교신저자Korea Institute of Materials Science (KIMS), 797, Changwondaero, Seongsan-gu, Changwon, Gyeongnam 641-010, Korea
초록
It was tried to find the optimal condition to prepare the metallic niobium powder with minimal oxygen content by atmospheric magnesium-gas reduction of niobium pentoxide (Nb2O5) powder at 1073-1223 K, which are industrially moderate and low temperature ranges until maximally 80 h inside the chamber held under the argon circumstances of 110 kPa. Magnesium oxide of the by-product of the reduction, was dissolved and removed fully by dissolving in a 10% aqueous hydrochloric acid solution. The particle size of the niobium powder reduced for 20 h was slightly increased within the range of 200 similar to 600nm according to increase of reduction temperatures. And such fine particles were further coarsened to near 1 mu m by increase of reduction times until 80 h at 1173 K, which is thought to be the most suitable for magnesium-gas reduction to be applied in industry. The reduction time satisfied for a maximal reduction effect was found to be 60 hours as the oxygen content was then minimally saturated to about 0.42 wt.%. Furthermore, the hydrogen contamination due to acid leaching of 0.28 wt.% was fully removed by dehydrogenation, which was a heat treatment performed under vacuum at 827K for 2 h; this resulted in the formation of metallic niobium powder.
키워드
niobium powdermagnesium reductionniobium pentoxide powdermagnesium oxidehydrochloric acid solutionniobium hydrideMAGNESIOTHERMIC REDUCTIONCALCIOTHERMIC REDUCTIONLATTICE-PARAMETERTANTALUMNANOPARTICLESEXPANSIONOXIDES