Densification of Mn-Doped YSZ for the Solid Oxide Membrane Process and its Surface Corrosion under Fluoride Salt
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q3Scopus Q3
- 저널
- JOURNAL OF CERAMIC SCIENCE AND TECHNOLOGY11(2) · pp.91 · 2020
- 피인용
- Web of Science 3Scopus 3
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2019 1.153
- ISSN
- 2190-9385
저자
- 조강희제1저자School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
- Buyoung, K.Department of Research and Development, HyMAR Corporation, Busan 46241, Republic of Korea
- Jiseung, R.Analysis Technology Center, Korea Institute of Ceramic Engineering and Technology, Jinju-si, Gyeongsangnam-do 52851, Republic of Korea
- Hyeong-Tae, K.Engineering Ceramic Center, Korea Institute of Ceramic Engineering and Technology, Icheon Branch Institute, Icheon-si, Gyeonggi-do 17303, Republic of Korea
- 이희수교신저자School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
초록
The densification-induced changes in the crystal structure and microstructure of x mol% Mn-doped 8YSZ (xMn-YSZ, x = 0, 0.5, 1.0, or 2.0) were investigated, and the mechanical and electrical properties of the samples were determined to evaluate their chemical degradation resulting from chemical stress loading. The xMn-YSZ samples synthesized with a solid-state reaction method possessed cubic crystal structures, similar to 8YSZ. The 0.5Mn-YSZ (111) peak shifted to a lower angle compared to that of YSZ. As the content of Mn increased, the xMn-YSZ peak gradually shifted to higher angles. The peak shift was attributed to lattice shrinkage (after expansion) with increasing Mn content. The grain size and porosity of YSZ were 9.07 mu m and 1.21 %, respectively, and those of 0.5Mn-YSZ were 21.90 mu m and 0.63 % respectively, revealing that Mn doping led to densification. The hardness increased to 2065.92 Hv (2.0Mn-YSZ) with increasing Mn content, similar to density. Because of the complex effects of densification and lattice distortion, the polarization resistance decreased to 48 % of YSZ for 0.5Mn-YSZ; however, the resistance gradually increased with increasing Mn content. After NaF-CaF2 was loaded as a chemical stress, the cubic and tetragonal phases destabilized and the porosity increased to 2.80 % and 5.44 % for 1.0Mn-YSZ and 2.0Mn-YSZ, respectively. On the other hand, 0.5Mn-YSZ without the tetragonal phase showed a porosity of 2.25 %, indicating that a Mn doping content of > 2.0 mol% worsened YSZ corrosion.
키워드
Mn-doped YSZsinterabilitypolarization resistancefluoride saltsurface corrosiondestabilizationYTTRIA-STABILIZED-ZIRCONIAMICROSTRUCTURERESISTANCE