본문 바로가기

Effect of pre-deformation before aging on discontinuous precipitation behaviour in Cu-Ni-Si alloys

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q4Scopus Q3
저널
PHILOSOPHICAL MAGAZINE LETTERS101(2) · pp.51 · 2021
피인용
Web of Science 23Scopus 24
FWCI (Scopus)
1.02
JCR IF
JCR 2020 0.909
ISSN
0950-0839

저자

  1. Cao, Yicheng제1저자State Key Laboratory of Nonferrous Metals and Processes, GRINM Group Co, Beijing, People's Republic of China
  2. Han, Seung Zeon교신저자Materials Processing Innovation Research Division, Korea Institute of Materials Science, Changwon, Korea
  3. Choi, Eun-AeMaterials Processing Innovation Research Division, Korea Institute of Materials Science, Changwon, Korea
  4. Ahn, Jee HyukMaterials Processing Innovation Research Division, Korea Institute of Materials Science, Changwon, Korea
  5. Mi, XujunState Key Laboratory of Nonferrous Metals and Processes, GRINM Group Co, Beijing, People's Republic of China
  6. Huang, GuojieState Key Laboratory of Nonferrous Metals and Processes, GRINM Group Co, Beijing, People's Republic of China
  7. 이상진Department of Materials Engineering, Pusan National University, Pusan, Korea
  8. Shin, HyeonseokMaterials Processing Innovation Research Division, Korea Institute of Materials Science, Changwon, Korea
  9. Kim, SangshikDepartment of Materials Science and Engineering, RECAPT, Gyeongsang National University, Chinju, Korea
  10. Lee, JehyunDepartment of Materials Science and Engineering, Changwon National University, Changwon, Korea

초록

The effect of deformation before aging on discontinuous precipitation in Cu-4.75wt%Ni-1.13wt%Si and Cu-6wt%Ni-1.42wt%Si alloys after solution treatment was investigated. Two kinds of deformation, one under and the other over the uniform deformation limit were implemented after solution treatment. With increasing deformation strain in both alloys, the discontinuous precipitation is accelerated and the aging time for a fully covered region by discontinuous precipitation is shortened. However, the Cu-6wt%Ni-1.42wt%Si alloy deformed under the uniform deformation limits showed an enhanced discontinuous precipitation compared to that for the alloy deformed over the uniform deformation limit. The deformation defects including dislocations and shear bands play the role of encouraging discontinuous precipitation. The shear bands formed during prior deformation beyond the necking point could provide sites for discontinuous precipitation initiation in the early stages of annealing However, shear bands tend to hinder the advance of discontinuous precipitation with further aging in the Cu-Ni-Si alloy with a high content of Ni and Si.

키워드

Cu-Ni-Si alloydiscontinuous precipitationNi2Siprior-deformation before agingslip bands shear bandsMICROSTRUCTURECONDUCTIVITYDISLOCATIONSDIFFUSIVITYSTRENGTH

식별자

Scopus EID
2-s2.0-85096558865
WoS UID
000591485100001