Structure and Physical Properties of Hydrophilic Polyamide Copolymers Fiber Based on Nylon 6 and Nylon 4,6
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q1Scopus Q2
- 저널
- Fibers and Polymers21(10) · pp.2173 · 2020
- 피인용
- Web of Science 12Scopus 13KCI 1
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2019 1.797
- ISSN
- 1229-9197
저자
- 김민석제1저자Department of Organic Material Science and Engineering, Pusan National University, Busan, 46241, Korea
- Hwang, Yeong NamKolon Industries, Inc., Gumi, 39366, Korea
- Kwon, Soon TaekKorea Textile Development Institute, Daegu, 41842, Korea
- 이승걸교신저자Department of Organic Material Science and Engineering, Pusan National University, Busan, 46241, Korea
- 조현혹교신저자Department of Organic Material Science and Engineering, Pusan National University, Busan, 46241, Korea
초록
Recently, hydrophilic synthetic fiber products have been sought to substitute natural fibers. This paper investigates the structure and properties of spined copolymer of nylon 6, nylon 4,6 and polyethylene oxide (PEO) - polypropylene oxide (PPO) diamine according to contents of PEO-PPO diamine (15-40%). The structure of new polyamide (NPA) were analyzed by X-ray diffraction (XRD), differential scanning calorimeter (DSC), dynamic mechanical analysis (DMA), gradient density column and gas pycnometry. Through XRD and DSC analysis, it was confirmed that the structure of NPA was similar to nylon 6 regardless of the content of PEO-PPO diamine. The DMA results show that the mobility of polymer chain in non-crystalline structure increases. It was considered that PEO-PPO diamine provides flexible segments and hydrophilic moieties to NPA. The analysis of moisture regain and tenacity was revealed that NPA exhibited 7.38% moisture regain and 2.85 g/denier tenacity.
키워드
Nylon 6Nylon 4,6CopolymerPoly(ethylene oxide) diamineMoisture regainPOLYETHYLENE OXIDE
식별자
- Scopus EID
- 2-s2.0-85094631097
- WoS UID
- 000583056800003
- KCI
- ART002637640



로그인
연구물 목록으로