Cu-6 wt% Ni-1.4 wt% Si 합금의 압연 후 기계적 성질에 미치는 시효전 처리 영향
Effect of Pre-Aging Treatment on the Mechanical Properties of Cold Rolled Cu-6 wt% Ni-1.4 wt% Si Alloy
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q3Scopus Q2
- 저널
- Korean Journal of Metals and Materials58(7) · pp.488 · 2020
- 피인용
- Web of Science 6Scopus 6KCI 2
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2019 1.146
- ISSN
- 1738-8228
저자
- 이상진제1저자School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
- Shin, Hyeon SeokMaterials Processing Innovation Research Division, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- Choi, Eun-AeMaterials Processing Innovation Research Division, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- Ahn, Jee HyukMaterials Processing Innovation Research Division, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- 최윤석교신저자School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
- Kim, SangshikDept. of Materials Engineering and Convergence Technology, ReCAPT Gyeongsang National University, Jinju 52828, Republic of Korea
- Lee, JehyunDepartment of Materials Science and Engineering, Changwon National University, Changwon 51140, Republic of Korea
- Han, Seung Zeon교신저자Materials Processing Innovation Research Division, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
초록
Cu-Ni-Si alloys were strengthened by Ni2Si intermetallic compound precipitation in a Cu matrix during aging. The Cu-6 wt% Ni-1.4wt%Si alloy was prepared by water quenching (solution treatment) or air cooling (homogenization treatment) after heating 980 degrees C for 2 hours and aging at 500 degrees C for 6 hours. After maintaining a high temperature single phase region, the structure of the precipitate in the matrix was changed significantly by varying the cooling rate. The solution treated aged alloy had discontinuous precipitation with fiber shaped precipitates throughout the specimen, however, the alloy with homogenization had normal spherical shaped particles. The aged alloy after homogenization treatment had higher strength, ductility and electrical conductivity, of 628 MPa, 18%, 48% IACS, respectively, than aged alloy after solution treatment, which had 582 MPa, 15.5% and 50 % IACS, respectively. In contrast to the tendency of values after aging, after rolling and a 75% area reduction at room temperature after homogenization treatment the alloy had lower strength, ductility and electrical conductivity, of 774 MPa, 10.5%, 48% IACS, than the alloy after solution treatment, with 885 MPa, 6.5%, and 48% IACS, respectively. The Cu-6 wt% Ni-1.4wt%Si alloy with fully discontinuous precipitation had lower strength and higher electrical conductivity than the counterpart alloy with normal precipitation. However, inversely, the strength increased compared to the alloy with normal precipitation after rolling with 75% area reduction, without sacrificing electrical conductivity.
키워드
Cu-Ni-Si alloyagingNi2Si intermetallic compoundprecipitation hardeningelectrical conductivitynormal precipitationdiscontinuous precipitationDISCONTINUOUS PRECIPITATIONELECTRICAL-CONDUCTIVITYHIGH-STRENGTHDEFORMATIONMICROSTRUCTUREBEHAVIOR
식별자
- Scopus EID
- 2-s2.0-85093837344
- WoS UID
- 000549095600007
- KCI
- ART002606131



로그인
연구물 목록으로