열간가공된 TiAl 합금의 미세조직 제어가 기계적 특성에 미치는 영향
Effect of Microstructure Control on the Mechanical Properties of Hot Worked TiAl Alloy
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q3Scopus Q2
- 저널
- Korean Journal of Metals and Materials58(7) · pp.459 · 2020
- 피인용
- Web of Science 7Scopus 7KCI 4
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2019 1.146
- ISSN
- 1738-8228
저자
- 김종훈제1저자School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
- Kim, Jae-KwonTitanium Department, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- Kim, Seong-Woong교신저자Titanium Department, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- 박용호School of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
- Kim, Seung EonTitanium Department, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
초록
The microstructure and mechanical properties of a newly developed, beta-phase containing TiAl alloy have been studied through hot working and post heat treatment to enhance room temperature ductility and strength. The controlled microstructures hadthree types of structure, fully lamellar, nearly lamellar and duplex, and were produced by cyclic heat-treatment in a single a region and (alpha+gamma) region after a hot-forging process in high temperature (alpha+beta) region. As a result of the room temperature tensile test, the fully lamellar structure exhibited a tensile strength of 622 MPa and ductility of 0.62%. The duplex structure had a tensile strength of 787 MPa and ductility of 1.22%, while the nearly lamellar structure showed a tensile strength of 880 MPa and ductility of 1.76%. In the room temperature tensile test, the nearly lamellar structure exhibited excellent tensile strength and ductility. The strength and ductility were increased by decreasing grain size and beta / B2 phase fraction. The newly developed TiAl alloy showed higher tensile values compared with the previous TiAl alloys. The relationship between microstructure and room temperature tensile properties of the newly developed beta-phase containing TiAl alloy was examined, and the best approach for hot working and post heat-treatment to obtain the most balanced mechanical properties was proposed.
키워드
gamma-TiAlheat treatmenthot workingmicrostructureductilityHIGH NBDYNAMIC RECRYSTALLIZATIONTENSILE PROPERTIESGRAIN-SIZEEVOLUTIONBEHAVIORCREEPDEFORMATIONDESIGNFRACTIONγ-TiAl