Fabrication of porous titanium parts by powder bed fusion of Ti-TiH2 blended powder
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q2
- 저널
- JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T9(3) · pp.3026 · 2020
- 피인용
- Web of Science 16Scopus 16
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2019 5.289
- ISSN
- 2238-7854
저자
- 윤혜정제1저자School of Mechanical Engineering, Pusan National University, Busan 46241, Republic of Korea
- 다니얄 아볼하사니Department of Mechanical Engineering, University of Birjand, Birjand 97175-376, Iran
- 황태우School of Mechanical Engineering, Pusan National University, Busan 46241, Republic of Korea
- 이태경School of Mechanical Engineering, Pusan National University, Busan 46241, Republic of Korea
- 김지훈School of Mechanical Engineering, Pusan National University, Busan 46241, Republic of Korea
- 문영훈교신저자School of Mechanical Engineering, Pusan National University, Busan 46241, Republic of Korea
초록
When a high-energy laser is used to irradiate Ti-chi TiH2 blended powder, hydrogen gas (H2) is generated by the decomposition of the titanium hydride (TiH2) powder and serves as a pore former and active agent. In this study, the powder bed fusion (PBF) of Ti-chi TiH2 (chi = 2, 5, 10 wt.%) blended powder was used to innovatively fabricate porous titanium parts. The trapped H-2 in the rapidly solidified molten pool produces porosity in the deposited layer. The PBF test results showed that the beam interaction time to generate H-2 through the decomposition of TiH2 is important in controlling the porosity formation. As the content of TiH2 increases, the porosity increases owing to the increased amount of H-2 generated from TiH2. Additionally, the porosity increases with increasing scan rate. The faster the scan rate, the more H-2 is trapped, because the rapidly solidified molten pool does not provide sufficient time for H-2 to diffuse out. The variation in porosity with subsequent layering in the PBF process was also investigated. The results of this study show that the porosity can be actively controlled by adjusting the TiH2 mixing ratio (chi) and the laser-processing parameters. (C) 2020 The Authors. Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (httplicreativecommens.org/licenses/by-ne-nd/4.0/).
키워드
Powder bed fusionSelective laser meltingPorosityTitaniumTitanium hydrideTI SCAFFOLDSLASERMICROSTRUCTUREPARAMETERSPOROSITYALLOYLAYERSTEEL