Early hydration and hardening of OPC-CSA blends for cementitious structure of 3D printing
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q2
- 저널
- ADVANCES IN APPLIED CERAMICS119(7) · pp.393 · 2020
- 피인용
- Web of Science 22Scopus 11
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2019 1.669
- ISSN
- 1743-6753
저자
- 김성훈제1저자School of Materials Science and Engineering, Pusan National University, Busan, Republic of Korea
- 김태우School of Materials Science and Engineering, Pusan National University, Busan, Republic of Korea
- Kim, BuyoungDepartment of research and development, HyMAR Corporation, Busan, Republic of Korea
- Kim, Hong-daeGreen Materials & Process Group, Korea Institute of Industrial Technology, Ulsan, Repulic of Korea
- Kim, JaeyoungCollege of Global Business, Korea University, Sejong City, Republic of Korea
- 이희수교신저자School of Materials Science and Engineering, Pusan National University, Busan, Republic of Korea
초록
The buildability of cementitious structure for 3D printing was investigated in terms of ettringite formation and hardening behaviour with packing density of OPC-CSA blends. The packing density of the OPC was 2.34 g cm(-3), increased to 2.39 g cm(-3)when 10 wt-% CSA was added, and then began to decrease to 2.37 g cm(-3)at 15 wt-% CSA addition. The exothermic peak was observed at around 114 degrees C which is the formation temperature of ettringite, and the exothermic value of ettringite was 2.42 mW mg(-1)(OPC), increased to 3.27 mW mg(-1)(CSA 10 wt-%), and then started to decrease from 2.72 mW mg(-1)(CSA 15 wt-%). For the quantitative analysis of ettringite formation, the amount of ettringite formation in OPC was 5.87%, but increased rapidly with the addition of CSA, showing the maximum value 9.49% at 10 wt-% CSA addition. The formation of needle-shaped ettringite was observed in all OPC-CSA blends, and the intertwined structures were appeared as the amount of ettringite formation increased. The flexural strength of OPC was 0.88 MPa, but increased rapidly according to the addition of CSA, and the maximum strength was 2.88 MPa at 10 wt-% CSA with the largest amount of ettringite formation.
키워드
OPC-CSA blendspacking densityettringiteflexural strengthbuildabilityORDINARY PORTLAND-CEMENTPACKING DENSITYETTRINGITEDESIGN
식별자
- Scopus EID
- 2-s2.0-85087116309
- WoS UID
- 000545330200001



로그인
연구물 목록으로