Recovery Behavior of Fe-Based Shape Memory Alloys under Different Restraints
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q2
- 저널
- APPLIED SCIENCES-BASEL10(10) · 2020
- 피인용
- Web of Science 29Scopus 33
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2019 2.474
- ISSN
- 2076-3417
저자
- Hong, Ki-Nam제1저자Department of Civil Engineering, Chungbuk National University, 1 Chungdae-ro, Seowon-Gu, Cheongju, Chungbuk 28644, Korea
- Yeon, Yeong-Mo교신저자Department of Civil Engineering, Chungbuk National University, 1 Chungdae-ro, Seowon-Gu, Cheongju, Chungbuk 28644, Korea
- Shim, Won-BoDepartment of Civil Engineering, Chungbuk National University, 1 Chungdae-ro, Seowon-Gu, Cheongju, Chungbuk 28644, Korea
- 김도형Department of Mechanical Engineering, Pusan National University, Busan 46241, Korea
초록
This paper presents the experimental results of an evaluation of the recovery behavior of Fe-based shape memory alloys (Fe-SMAs) under different restraints. For the study, three types of Fe-SMA (FSMA-A, FSMA-B, FSMA-C) were produced. As a result of the direct tensile test, the yield strength of the FSMA-A specimen was nearly 34% higher than the strength of FSMA-B and FSMA-C. Under free restraint, the recovery strains are 0.00956, 0.01445, and 0.01977 for FSMA-A, FSMA-B and FSMA-C specimens, respectively, after activation when the pre-strain is 0.04, and the heating temperature 200 degrees C. Under rigid restraint, the final recovery stresses are 518, 391 and 401 MPa for FSMA-A, FSMA-B, FSMA-C specimens after activation when a pre-strain of 0.04 and heating temperature 200 degrees C. Additionally, under the rigid restraint, the effect of pre-strain on the final recovery stress was insignificant, whereas the final recovery stress increased as the heating temperature increased. When Fe-SMA was constrained during cooling, the recovery stress is 50% lower than under rigid restraint. Hence, in order to develop a large recovery stress, Fe-SMA must be constrained during heating. In addition, a method for calculating the effective confining stress of the Fe-SMA coupler for pipe joining was proposed based on the experimental results.
키워드
Fe-based shape memory alloy (Fe-SMA)recovery stressactivationrestraintpre-strainheating temperaturepipe joiningTRANSFORMATIONSTRIPSSTRESS
식별자
- Scopus EID
- 2-s2.0-85085691729
- WoS UID
- 000541440000102



로그인
연구물 목록으로