Room-temperature synthesis and CO2-gas sensitivity of bismuth oxide nanosensors

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q2Scopus Q1
저널
RSC ADVANCES10(29) · pp.17217 · 2020
피인용
Web of Science 42Scopus 45
FWCI (Scopus)
0
JCR IF
JCR 2019 3.119
ISSN
2046-2069

저자

  1. Shinde, Pritamkumar V.제1저자Global Frontier R&D Centre for Hybrid Interface Materials, Pusan National University, 30, Jangjeon-dong, Geumjung-gu, Busan 609-735, Republic of Korea
  2. 신데National Core Research Centre, Pusan National University, 30, Jangjeon-dong, Geumjung-gu, Busan 609-735, Republic of Korea
  3. Shaikh, Shoyebmohamad F.Department of Chemistry, College of Science, King Saud University, Riyadh 11451, Saudi Arabia
  4. 이다민School of Materials Science and Engineering, Pusan National University, 30, Jangjeon-dong, Geumjung-gu, Busan 609-735, Republic of Korea
  5. 윤재무National Core Research Centre, Pusan National University, 30, Jangjeon-dong, Geumjung-gu, Busan 609-735, Republic of Korea
  6. 이정우School of Materials Science and Engineering, Pusan National University, 30, Jangjeon-dong, Geumjung-gu, Busan 609-735, Republic of Korea
  7. Al-Enizi, Abdullah M.교신저자Department of Chemistry, College of Science, King Saud University, Riyadh 11451, Saudi Arabia
  8. 라자람 사카람 마네Global Frontier R&D Centre for Hybrid Interface Materials, Pusan National University, 30, Jangjeon-dong, Geumjung-gu, Busan 609-735, Republic of Korea
  9. 김광호Global Frontier R&D Centre for Hybrid Interface Materials, Pusan National University, 30, Jangjeon-dong, Geumjung-gu, Busan 609-735, Republic of Korea

초록

Room-temperature (27 degrees C) synthesis and carbon dioxide (CO2)-gas-sensor applications of bismuth oxide (Bi2O3) nanosensors obtained via a direct and superfast chemical-bath-deposition method (CBD) with different surface areas and structures, i.e., crystallinities and morphologies including a woollen globe, nanosheet, rose-type, and spongy square plate on a glass substrate, are reported. Moprhologies of the Bi2O3 nanosensors are tuned through polyethylene glycol, ethylene glycol, and ammonium fluoride surfactants. The crystal structure, type of crystallinity, and surface appearance are determined from the X-ray diffraction patterns, X-ray photoelectron spectroscopy spectra, and high-resolution transmission electron microscopy images. The room-temperature gas-sensor applications of these Bi2O3 nanosensors for H-2, H2S, NO2, SO2, and CO2 gases are monitored from 10 to 100 ppm concentrations, wherein Bi2O3 nanosensors of different physical properties demonstrate better performance and response/recovery time measurement for CO2 gas than those for the other target gases employed. Among various sensor morphologies, the nanosheet-type Bi2O3 sensor has exhibited at 100 ppm concentration of CO2 gas, a 179% response, 132 s response time, and 82 s recovery time at room-temperature, which is credited to its unique surface morphology, high surface area, and least charge transfer resistance. This suggests that the importance of the surface morphology, surface area, and crystallinity of the Bi2O3 nanosensors used for designing room-temperature operable CO2 gas sensors for commercial benefits.

키워드

GAS-SENSING PROPERTIESWET-CHEMICAL-SYNTHESISOPTICAL-PROPERTIESNANOWIRE ARRAYSENSORSNO2NANOSTRUCTURESMORPHOLOGIESPERFORMANCESMICROSPHERES